Abstract

Abstract The recoverability by cyanidation of the gold content of sedimentary gold-bearing ores containing organic carbonaceous material and gold-bearing pyrite, or other gold-bearing sulfides, is greatly increased by heating an aqueous slurry of the ore to about 167° to 212° F. and then introducing air or oxygen into the heated slurry to oxidize and eliminate a substantial portion of the carbonaceous material and oxidizable sulfides in the slurried ore, followed by cooling the slurry to about 70° to 85° F. and then introducing chlorine gas into the slurry to substantially complete the oxidation and chlorination of the carbonaceous content of the slurried ore. The ore is then subjected to conventional cyanidation to recover the gold content thereof.

Inventors

  • 👤 Wilbur J. Guay

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 01:46
CPC Classifications
C; C22; C22B; C22B11/00; C22B11/08; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 223 words
The method for treating sedimentary gold-bearing ore containing indigenous organic carbonaceous material and gold-bearing sulfides so as to increase the recoverability of its gold content by standard cyanidation extraction which comprises: slurrying the ore with water in the absence of extraneous alkaline material; adjusting the temperature of the slurry to about 167° to 212° F., and dispersing air or oxygen throughout the slurry at a rate and for a period of time such as the slurry will continue to absorb oxygen as the oxygen reacts with the organic carbonaceous components and the sulfice content of the ore; adjusting the temperature of the slurry to about 70° to 85° F., and dispersing chlorine gas throughout the slurry at a rate and for a period of time such as the slurry will continue to absorb the chlorine with evolution of carbon dioxide, nitrogen, and oxygen, as the chlorine reacts with the organic carbonaceous components of the ore and only until a significant amount of chlorine gas is liberated from the chlorinated slurry; and maintaining the thus chlorinated slurry at a temperature within the range of about 70° to 85° F. for a period of about 6 to 12 hours with the resulting production of a slurry-solids content in which the gold component is amenable to at least 75 weight percent extraction by standard cyanidation practice.
Claim 2
Independent Claim 223 words
The method for treating sedimentary gold-bearing ore containing indigenous organic carbonaceous material and gold-bearing sulfides so as to increase the recoverability of its gold content by standard cyanidation extraction which comprises: slurrying the ore with water in the absence of extraneous alkaline material; adjusting the temperature of the slurry to about 167° to 212° F., and dispersing air or oxygen throughout the slurry at a rate and for a period of time such as the slurry will continue to absorb oxygen as the oxygen reacts with the organic carbonaceous components and the sulfice content of the ore; adjusting the temperature of the slurry to about 70° to 85° F., and dispersing chlorine gas throughout the slurry at a rate and for a period of time such as the slurry will continue to absorb the chlorine with evolution of carbon dioxide, nitrogen, and oxygen, as the chlorine reacts with the organic carbonaceous components of the ore and only until a significant amount of chlorine gas is liberated from the chlorinated slurry; and maintaining the thus chlorinated slurry at a temperature within the range of about 70° to 85° F. for a period of about 6 to 12 hours with the resulting production of a slurry-solids content in which the gold component is amenable to at least 75 weight percent extraction by standard cyanidation practice.
Claim 3
Dependent Claim 28 words
The method according to claim 1 in which the air or oxygen is dispersed throughout the heated slurry for a period of between about 8 to 24 hours.
Claim 4
Dependent Claim 26 words
The method according to claim 1 in which the chlorine gas is dispersed throughout the slurry for a period of between about 6 to 12 hours.

References Cited (Backward Citations)

US1734306A Cited
US2777764A Cited
US3574600A Cited
US3846124A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-07-25 1981-01-24 1981-07-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-07-25 1985-01-24 1985-07-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-07-25 1989-01-24 1989-07-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag