Apparatus for the continuous application of a metallic coating to a metal strip
Assignee: Individual
•
Filing: 1975-04-22
•
Granted: 1977-07-19
•
Expires: 1995-04-22
Abstract
Abstract Steel strip is continuously coated with molten metal by passing it through a plasma arc and projecting the molten metal thereon in an inert atmosphere, e.g. nitrogen. The projecting means reciprocates transversely of the strip. The strip is preheated prior to deposition and the surface of the coating is reheated for refusion of only the surface of the coating. An inert atmosphere is maintained in an enclosure surrounding the projecting apparatus, by directing inert gas against the coated strip in a direction opposite to the direction of movement of the strip.
Inventors
- 👤 Felix Montbrun
- 👤 Roland Liesenborghs
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 19:21
CPC Classifications
C; C23; C23C; C23C4/00; C23C4/12; C23C4/14; B; B05; B05B; B05B13/00; B05B13/02; B05B13/04; B05B13/0463; B05B13/0468; B05B13/0473; C23C4/18
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
106 words
Apparatus for the continuous application of a metallic coating to a metal strip, comprising: an airtight enclosure, means for continuously advancing the metal strip lengthwise of itself through said enclosure at least one plasma torch for projecting molten metal onto the continuously advancing metal strip a trolley carrying said plasma torch fixed rails carrying said trolley and extending parallel to the plane of said metal strip and perpendicular to the longitudinal direction thereof means for reciprocating said trolley with said plasma torch, on said rails, within said enclosure across the entire width of said metal strip and means for maintaining an inert atmosphere in said enclosure.
Claim 2
Dependent Claim
106 words
Apparatus for the continuous application of a metallic coating to a metal strip, comprising: an airtight enclosure, means for continuously advancing the metal strip lengthwise of itself through said enclosure at least one plasma torch for projecting molten metal onto the continuously advancing metal strip a trolley carrying said plasma torch fixed rails carrying said trolley and extending parallel to the plane of said metal strip and perpendicular to the longitudinal direction thereof means for reciprocating said trolley with said plasma torch, on said rails, within said enclosure across the entire width of said metal strip and means for maintaining an inert atmosphere in said enclosure.
Claim 3
Dependent Claim
64 words
Apparatus according to claim 1, further comprising means for introducing inert gas with means for directing said gas against and along the coated face of said metal strip towards the jet issued from said at least one plasma torch, said gas controlling the atmosphere near said coated face of said metal strip in order to regulate the state of oxidation of the applied coating.
Claim 4
Dependent Claim
37 words
Apparatus according to claim 1, further comprising: a preheating enclosure located upstream of said airtight enclosure, and electrical heating means for preheating said metal strip in said preheating enclosure prior to its introduction into said airtight enclosure.
Claim 5
Dependent Claim
41 words
Apparatus according to claim 1, further comprising: a refusion enclosure located downstream said projecting enclosure, and electrical means for heating and partially remelting the coating of said coated metal strip into said refusion enclosure after its passage through said projecting enclosure.
Claim 6
Dependent Claim
38 words
Apparatus according to claim 4, further comprising: a cooling chamber located downstream of said refusion enclosure, and cooling means for cooling the coating of said metal strip in said cooling chamber after its passage through said refusion enclosure.
References Cited (Backward Citations)
US2250561A
Cited
US2746420A
Cited
US3010009A
Cited
US3071678A
Cited
US3325620A
Cited
US3211886A
Cited
US3440390A
Cited
US3394678A
Cited
US3839618A
Cited
US3819901A
Cited
US3900639A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-07-18 | 1981-01-17 | 1981-07-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-07-18 | 1985-01-17 | 1985-07-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-07-18 | 1989-01-17 | 1989-07-19 | $7700.00 | Window Closed / Lapsed |