Laminating method for producing pressure-sensitive adhesive coated substrates having a release layer affixed thereto

Assignee: Spinnaker Coating Inc
•
Filing: 1976-03-15
•
Granted: 1977-07-12
•
Expires: 1996-03-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for producing releasable laminates by coating a water-dispersed pressure-sensitive adhesive onto either a web of paper face stock or a web of release paper, joining the two webs together with the adhesive therebetween while the adhesive is still wet, and then drying under moderate conditions to produce a relatively wrinkle-free and flat laminate having an exceptionally smooth and uniform adhesive layer.

Inventors

  • 👤 Roger E. Yount

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 10:53
CPC Classifications
D; D21; D21H; D21H27/00; D21H27/001

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 190 words
A method for producing releasable laminates having a paper substrate coated with a tacky pressure-sensitive adhesive and a release layer releasably affixed to the pressure-sensitive adhesive comprising: (a) providing a web of paper face stock, (b) providing a web of moisture sensitive or absorptive release paper having a release material coated thereon, (c) coating either said web of paper face stock or the previously coated side of said web of release paper with a water-dispersed pressure-sensitive adhesive, (d) before drying, joining the webs together with the still-wet adhesive therebetween, (e) passing the joined webs through a pressure nip to form a laminate, then (f) drying said laminate to a relative humidity of around 30-60% (Cambridge Moisture Indicator test) so as to allow for a moisture equilibration between said webs, (g) winding said laminate on a roll, and (h) conditioning said laminate for a period of time prior to further processing to allow for additional moisture equilibration between said webs, whereby there is produced a laminate having a pressure-sensitive adhesive coated substrate and a release layer thereover, said adhesive being smooth and uniform and said laminate being relatively wrinkle-free and flat.
Claim 2
Independent Claim 190 words
A method for producing releasable laminates having a paper substrate coated with a tacky pressure-sensitive adhesive and a release layer releasably affixed to the pressure-sensitive adhesive comprising: (a) providing a web of paper face stock, (b) providing a web of moisture sensitive or absorptive release paper having a release material coated thereon, (c) coating either said web of paper face stock or the previously coated side of said web of release paper with a water-dispersed pressure-sensitive adhesive, (d) before drying, joining the webs together with the still-wet adhesive therebetween, (e) passing the joined webs through a pressure nip to form a laminate, then (f) drying said laminate to a relative humidity of around 30-60% (Cambridge Moisture Indicator test) so as to allow for a moisture equilibration between said webs, (g) winding said laminate on a roll, and (h) conditioning said laminate for a period of time prior to further processing to allow for additional moisture equilibration between said webs, whereby there is produced a laminate having a pressure-sensitive adhesive coated substrate and a release layer thereover, said adhesive being smooth and uniform and said laminate being relatively wrinkle-free and flat.
Claim 3
Dependent Claim 45 words
The method of claim 1 wherein said drying step takes place in a drier providing gradient drying, and the speed of throughput for the laminate being relatively slow so as to produce around 30-60% relative humidity (Cambridge Moisture Indicator test) on exit from said drier.
Claim 4
Dependent Claim 25 words
The method of claim 2 wherein said temperature is in a gradient from ambient to 120°-180° F. and said speed is 100-300 feet per minute.
Claim 5
Dependent Claim 26 words
The method of claim 3 wherein said conditioning step is aging for approximately one to ten days at room temperature and pressure prior to further processing.
Claim 6
Dependent Claim 70 words
The method of claim 1 wherein said paper face stock is selected from the group consisting of fluorescent paper, kraft paper, English finish paper, coated one or two side litho, cast coated face stock, offset paper and highly calendered paper, and said adhesive is selected from the group consisting of acrylic ester-vinyl acetate copolymers, ethylene-vinyl acetate copolymers, plasticized vinyl acetate homopolymers, rubber latex-resin emulsions, and acrylic ester homopolymers and copolymers.
Claim 7
Dependent Claim 20 words
The method of claim 5 wherein said adhesive is a water-dispersed acrylic ester-vinyl acetate copolymer having approximately a 35-65% solids.
Claim 8
Dependent Claim 27 words
The method of claim 6 wherein said adhesive is coated onto said paper face stock within a coat weight range of about 10-22 lbs/ream (3300 sq. ft.).
Claim 9
Dependent Claim 52 words
The method of claim 7 wherein said laminate is dried by gradient drying ranging in temperature from ambient to 120°-180° F., said laminate is passed through said drier at the rate of 100-300 feet per minute, and said laminate exits from said drier at a 40-50% relative humidity (Cambridge Moisture Indicator test).
Claim 10
Dependent Claim 22 words
The method of claim 8 wherein said laminate is conditioned in roll form about one to ten days prior to further processing.

References Cited (Backward Citations)

US2453258A Cited
US3515630A Cited
US3532652A Cited
US3914484A Cited
US3767500A Cited
US3922464A Cited
US3962012A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-07-11 1981-01-10 1981-07-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-07-11 1985-01-10 1985-07-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-07-11 1989-01-10 1989-07-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag