US4030989A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Electrowinning process
Assignee: Anglonor SA
•
Filing: 1976-05-11
•
Granted: 1977-06-21
•
Expires: 1996-05-11
Abstract
Abstract Metals from sulfate leach solutions derived from sulfide ores are electrowon in a cell divided by a permionic membrane whereby metal pregnant solution is fed to the cathode compartment and sulfuric acid is generated in the anode compartment.
Inventors
- 👤 Milton Graham Montgomery Atmore
- 👤 Roy Duncan Macpherson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 09:01
CPC Classifications
C; C25; C25C; C25C1/00; C25C1/06; C25C1/08; C25C1/12
Claims Analysis
Total Claims: 19
Claim 1
Independent Claim
150 words
A process for the recovery of a metal from a sulphurous feed material containing the metal, which process comprises leaching the sulphurous feed material with an aqueous leach solution to form an aqueous metal-bearing solution containing sulphate ions and ions of the metal; removing solids from the metal-bearing solution; and thereafter electrowinning the metal from the metal-bearing solution in an electrolytic cell having an anode compartment containing an anode and a cathode compartment containing a cathode, said compartments being separated by an ion-permeable, substantially fluid-impermeable membrane, by flowing the metal-bearing solution through the cathode compartment and flowing an aqueous acidic anolyte through the anode compartment, a potential difference being maintained between the anode and the cathode so as to electrodeposit ions of the metal from the metal-bearing solution onto the cathode and to cause the passage of sulphate ions through the membrane from the cathode compartment to the anode compartment.
Claim 2
Dependent Claim
150 words
A process for the recovery of a metal from a sulphurous feed material containing the metal, which process comprises leaching the sulphurous feed material with an aqueous leach solution to form an aqueous metal-bearing solution containing sulphate ions and ions of the metal; removing solids from the metal-bearing solution; and thereafter electrowinning the metal from the metal-bearing solution in an electrolytic cell having an anode compartment containing an anode and a cathode compartment containing a cathode, said compartments being separated by an ion-permeable, substantially fluid-impermeable membrane, by flowing the metal-bearing solution through the cathode compartment and flowing an aqueous acidic anolyte through the anode compartment, a potential difference being maintained between the anode and the cathode so as to electrodeposit ions of the metal from the metal-bearing solution onto the cathode and to cause the passage of sulphate ions through the membrane from the cathode compartment to the anode compartment.
Claim 3
Dependent Claim
30 words
A process according to claim 1, wherein the sulphurous feed material containing the metal contains at least one metal selected from the group consisting of nickel, copper, cobalt and zinc.
Claim 4
Dependent Claim
37 words
A process according to claim 2, wherein the metal-bearing solution which is flowed through the cathode compartment(s) of the electrowinning cell contains from 20 to 150 grams per liter of the metal which is to be electrowon.
Claim 5
Dependent Claim
37 words
A process according to claim 3, wherein the metal-bearing solution which is flowed through the cathode compartment(s) of the electrowinning cell contains from 30 to 70 grams per liter of the metal which is to be electrowon.
Claim 6
Dependent Claim
22 words
A process according to claim 3, wherein the aqueous acidic anolyte contains from 5 to 150 grams per liter of sulphuric acid.
Claim 7
Dependent Claim
22 words
A process according to claim 5, wherein the aqueous acidic anolyte contains from 10 to 50 grams per liter of sulphuric acid.
Claim 8
Dependent Claim
60 words
A process according to claim 1, wherein the aqueous acidic anolyte is flowed around a circuit which includes the anode compartment of the electrolytic cell, and a proportion of the aqueous acidic anolyte is bled from the circuit while there is added to the circuit an aqueous fluid so that the composition of the aqueous acidic anolyte can be controlled.
Claim 9
Dependent Claim
13 words
A process according to claim 7, wherein the said aqueous fluid is water.
Claim 10
Dependent Claim
26 words
A process according to claim 1, wherein the metal bearing solution is purified after solids have been removed therefrom and before the metal is electrowon therefrom.
Claim 11
Dependent Claim
41 words
A process according to claim 1, wherein the metal-bearing solution is flowed through a plurality of cathode compartments of the electrowinning cell and wherein the aqueous acidic anolyte is flowed through a single, common anode compartment disposed about the cathode compartments.
Claim 12
Dependent Claim
33 words
A process according to claim 1, wherein at least a part of the metal-bearing solution is recycled to the leaching step after it has passed through the cathode compartment of the electrolytic cell.
Claim 13
Dependent Claim
17 words
A process according to claim 1, wherein the ion-permeable, substantially fluid-impermeable membrane is an anion exchange membrane.
Claim 14
Dependent Claim
40 words
A process according to claim 1, wherein the cathode compartment comprises a substantially fluid-impermeable housing with an inlet and an outlet for the metal-bearing solution and with at least one wall of the housing constituted by an anion exchange membrane.
Claim 15
Dependent Claim
225 words
A process for the recovery of a metal from a sulphurous feed material containing the metal, which process comprises leaching the sulphurous feed material with an aqueous acidic leach solution to form an aqueous metal-bearing solution containing sulphate ions and ions of the metal; removing solids from the metal-bearing solution; and thereafter electrowinning the metal from the metal-bearing solution in an electrolytic cell having a cathode compartment containing a cathode and an anode compartment containing an anode and disposed about the cathode compartment, said compartments being separated by a substantially fluid-impermeable anion exchange membrane, by flowing the metal-bearing solution through the cathode compartment and flowing an aqueous acidic anolyte around a circuit which includes the anode compartment of the electrolytic cell and in which a proportion of the aqueous acidic anolyte is bled from the circuit while water is added to the circuit so that the composition of the aqueous acidic anolyte can be controlled, a potential difference being maintained between the anode and the cathode so as to electrodeposit ions of the metal from the metal-bearing solution onto the cathode and to cause the passage of sulphate ions through the membrane from the cathode compartment to the anode compartment, wherein a part of the metal-bearing solution is recycled to the leaching step after it has passed through the cathode compartment of the electrolytic cell.
Claim 16
Dependent Claim
225 words
A process for the recovery of a metal from a sulphurous feed material containing the metal, which process comprises leaching the sulphurous feed material with an aqueous acidic leach solution to form an aqueous metal-bearing solution containing sulphate ions and ions of the metal; removing solids from the metal-bearing solution; and thereafter electrowinning the metal from the metal-bearing solution in an electrolytic cell having a cathode compartment containing a cathode and an anode compartment containing an anode and disposed about the cathode compartment, said compartments being separated by a substantially fluid-impermeable anion exchange membrane, by flowing the metal-bearing solution through the cathode compartment and flowing an aqueous acidic anolyte around a circuit which includes the anode compartment of the electrolytic cell and in which a proportion of the aqueous acidic anolyte is bled from the circuit while water is added to the circuit so that the composition of the aqueous acidic anolyte can be controlled, a potential difference being maintained between the anode and the cathode so as to electrodeposit ions of the metal from the metal-bearing solution onto the cathode and to cause the passage of sulphate ions through the membrane from the cathode compartment to the anode compartment, wherein a part of the metal-bearing solution is recycled to the leaching step after it has passed through the cathode compartment of the electrolytic cell.
Claim 17
Dependent Claim
41 words
A process according to claim 14, wherein the metal-bearing solution is flowed through a plurality of cathode compartments of the electrowinning cell and wherein the aqueous acidic anolyte is flowed through a single, common anode compartment disposed about the cathode compartments.
Claim 18
Dependent Claim
40 words
A process according to claim 14, wherein the cathode compartment comprises a substantially fluid-impermeable housing with an inlet and an outlet for the metal-bearing solution and with at least one wall of the housing constituted by an anion exchange membrane.
Claim 19
Dependent Claim
19 words
A process according to claim 14, wherein the metal is selected from the group consisting of copper and nickel.
References Cited (Backward Citations)
GB189321193A
Cited
US2810686A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-06-20 | 1980-12-20 | 1981-06-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-06-20 | 1984-12-20 | 1985-06-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-06-20 | 1988-12-20 | 1989-06-21 | $7700.00 | Window Closed / Lapsed |