Consolidation of dry formed webs

Assignee: Domtar Inc
•
Filing: 1975-06-20
•
Granted: 1977-06-07
•
Expires: 1995-06-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of forming a paper-like sheet from a dry formed web by pre-bonding the web thereby strengthening it sufficiently that it may traverse a conventional size press but without unduly inhibiting the ability of the web to be penetrated by a binder in a liquid carrier, applying said binder to the pre-bonded web, distributing said binder in said web in a size press at a pressure of 20-150 lbs/linear inch, a temperature of 15° - 80° C and a web speed of at least 50 ft/minute and drying the web to provide a bonded sheet.

Inventors

  • 👤 Roger George Davey

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 01:28
CPC Classifications
D; D21; D21H; D21H5/00; D21H5/26; D21H5/265; D21H5/2657; D21H25/00

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 234 words
A method of continuously making a dry formed consolidated sheet of paper comprising: a. dry forming fibres to form a continuous web, said fibres being predominantly discrete cellulose fibres previously liberated by chemical digestion of cellulosic material; b. continuously passing said web containing 4 to 25% moisture based on the weight of said fibres between a pair of press rolls at a pressure of 500 - 3,000 lbs. per lineal inch and prebonding said fibres together thereby to impart sufficient strength to said web to enable it to pass through the nip of a size press when said web is substantially saturated with a binder in a liquid carrier but without significantly imparting the ability of said web to be impregnated by said binder in said liquid carrier; c. continuously applying said binder in said liquid carrier to said prebonded web, the amount of said binder in said liquid carrier being sufficient to saturate said web in said nip; d. continuously passing said prebonded web through said nip of said size press at a nip pressure of 20 to 150 lbs. per linear inch and at a speed of at least 50 ft. per minute said binder in said liquid carrier being at a temperature of 15 - 80° C thereby to distribute said binder substantially uniformly throughout said web and; e. drying said web to form a continuous bonded consolidated sheet of paper.
Claim 2
Independent Claim 234 words
A method of continuously making a dry formed consolidated sheet of paper comprising: a. dry forming fibres to form a continuous web, said fibres being predominantly discrete cellulose fibres previously liberated by chemical digestion of cellulosic material; b. continuously passing said web containing 4 to 25% moisture based on the weight of said fibres between a pair of press rolls at a pressure of 500 - 3,000 lbs. per lineal inch and prebonding said fibres together thereby to impart sufficient strength to said web to enable it to pass through the nip of a size press when said web is substantially saturated with a binder in a liquid carrier but without significantly imparting the ability of said web to be impregnated by said binder in said liquid carrier; c. continuously applying said binder in said liquid carrier to said prebonded web, the amount of said binder in said liquid carrier being sufficient to saturate said web in said nip; d. continuously passing said prebonded web through said nip of said size press at a nip pressure of 20 to 150 lbs. per linear inch and at a speed of at least 50 ft. per minute said binder in said liquid carrier being at a temperature of 15 - 80° C thereby to distribute said binder substantially uniformly throughout said web and; e. drying said web to form a continuous bonded consolidated sheet of paper.
Claim 3
Dependent Claim 14 words
A method as defined in claim 1 wherein step (b) is at room temperature.
Claim 4
Dependent Claim 22 words
A method as defined in claim 1 wherein step (b) applies substantially uniform pressure across the web and is at room temperature.
Claim 5
Dependent Claim 26 words
A method as defined in claim 1 wherein said binder in said liquid carrier of step (c) is applied in the size press of step (d).
Claim 6
Dependent Claim 26 words
A method as defined in claim 1 wherein step (c) applies binder in the amount of between 2 and 20% based on the weight of fibre.
Claim 7
Dependent Claim 62 words
A method as defined in claim 1 wherein said binder applied in step (c) is selected from the group consisting of starch adhesives, animal glue adhesives and carboxymethyl cellulose type adhesives and is applied as a water solution in the size press of step (d) and in the amount of between 2 and 20% based on the weight of said cellulose fibres.
Claim 8
Dependent Claim 56 words
A method as defined in claim 1 wherein at least a part of said binder applied in step (c) is applied as a spray and the remainder of said binder is applied in the size press of step (d) with all of said binder being distributed in said web by said size press in step (d).

References Cited (Backward Citations)

US2872337A Cited
US2983627A Cited
US3230287A Cited
US3773587A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-06-06 1980-12-06 1981-06-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-06-06 1984-12-06 1985-06-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-06-06 1988-12-06 1989-06-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag