← Back to Patent Explorer
US4026719A Expired / Lapsed US ⏱️ 0.0 years remaining

Sulfur composition with mica

Assignee: Chevron USA Inc
•
Filing: 1975-11-13
•
Granted: 1977-05-31
•
Expires: 1995-11-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A composition containing sulfur, a sulfur plasticizer and mica. The composition is surprisingly strong even without glass fiber in the composition. The composition can be used as a coating formulation or as a binder.

Inventors

  • 👤 Milutin Simic

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 17:57
CPC Classifications
E; E02; E02D; E02D3/00; E02D3/12; C; C04; C04B; C04B28/00; C04B28/36; C08; C08G; C08G75/00; C08G75/14; C08G75/16; C08K; C08K3/00; C08K3/02; C08K3/06; C08K3/34; C09; C09D; C09D5/00; C09D5/34; C09K; C09K17/00; C09K17/40; C09K17/42

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 21 words
A composition comprising 50-98 weight percent sulfur, 0.2 to 20 weight percent sulfur plasticizer, and 5 to 20 weight percent mica.
Claim 2
Dependent Claim 21 words
A composition comprising 50-98 weight percent sulfur, 0.2 to 20 weight percent sulfur plasticizer, and 5 to 20 weight percent mica.
Claim 3
Dependent Claim 18 words
A composition in accordance with claim 1 wherein the amount of mica is 5 to 20 weight percent.
Claim 4
Dependent Claim 75 words
A composition in accordance with claim 1 wherein the plasticizer is an aliphatic linear polysulfide; dioctylphthalate; acrylic acid; dicyclopentadiene; tall oil fatty acids; styrene; or an aromatic polysulfide formed by reacting one mol of an aromatic carbocyclic or a heterocyclic compound, substituted by at least one functional group of the class --OH or --NHR in which R is H or lower alkyl, with at least two mols of sulfur; or mixture of the foregoing plasticizers.
Claim 5
Dependent Claim 12 words
A composition in accordance with claim 1 wherein the plasticizer is dicyclopentadiene.
Claim 6
Dependent Claim 28 words
A composition in accordance with claim 1 wherein the plasticizer is an aromatic polysulfide formed by reacting one mol of phenol with at least two mols of sulfur.
Claim 7
Dependent Claim 26 words
A composition in accordance with claim 3 wherein the plasticizer is an aliphatic polysulfide polymer which has the reoccuring unit ----SxCH.sub.2 CH.sub.2 OCH.sub.2 OCH.sub.2 CH.sub.2 Sx--
Claim 8
Dependent Claim 12 words
A composition in accordance with claim 1 wherein the mica contains potassium.
Claim 9
Dependent Claim 12 words
A composition in accordance with claim 1 wherein the mica is phlogopite.
Claim 10
Dependent Claim 12 words
A composition in accordance with claim 1 wherein the mica is muscovite.

References Cited (Backward Citations)

US3316115A Cited
US3453125A Cited
US3823019A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-05-30 1980-11-29 1981-05-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-05-30 1984-11-29 1985-05-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-05-30 1988-11-29 1989-05-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag