Lithographic developer replenishment process

Assignee: EIDP Inc
•
Filing: 1975-05-23
•
Granted: 1977-05-24
•
Expires: 1995-05-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Lithographic developer in an automatic photographic film processor is replenished from at least two stable solution concentrates. As each quantity of lithographic film is processed predetermined amounts of the solution concentrates and water are mixed and immediately added to the developer. The solution concentrates, stable before mixing, contain all the constituents needed to replenish the developer solution to maintain activity at a desired level. The amount of each solution concentrate is predetermined from the concentration of each solution concentrate and the quantity and developer requirements of the film. The frequency of replenishment is predetermined from the usage pattern.

Inventors

  • 👤 Charles Anthony Allen
  • 👤 Thomas Albert Bailey, III
  • 👤 Joseph Anthony Sincius

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 14:43
CPC Classifications
G; G03; G03C; G03C5/00; G03C5/26; G03C5/29; G03C5/31

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 238 words
In a process of developing imagewise-exposed lithographic film in a bath of lith developer solution contained in an automatic photographic film processor, said solution containing hydroquinone as the sole developing agent and having a low sulfite ion concentration characterized by a high sensitivity to pH, to bromide ion, and to sulfite concentration changes, and being subject to aging due to aerial oxidation and anaerobic degradation, and wherein pH and concentrations of hydroquinone and bromide ion are changed by the development process and wherein quantities of premixed replenishers are added to said bath to compensate for concentration changes due to development and to aging, the improvement comprising: replenishing said bath of lith developer solution to compensate for concentration changes due to development by repetitively adding to the developer solution as each quantity of film is developed, in combination: 1. a quantity of a stable solution concentrate A having a pH below 8 and consisting essentially of an aqueous solution of sufficient hydroquinone to replace that consumed during development of each quantity of film, 2. a quantity of stable solution concentrate B consisting essentially of a strongly basic aqueous solution having a pH above 9, and free of developing agent, the amount of concentrate B being sufficient to maintain the pH and constituent concentration of the developer; and wherein A, B, or A+B contains sodium formaldehyde bisulfite in an amount sufficient to act as a buffer for sulfite ion concentration.
Claim 2
Dependent Claim 238 words
In a process of developing imagewise-exposed lithographic film in a bath of lith developer solution contained in an automatic photographic film processor, said solution containing hydroquinone as the sole developing agent and having a low sulfite ion concentration characterized by a high sensitivity to pH, to bromide ion, and to sulfite concentration changes, and being subject to aging due to aerial oxidation and anaerobic degradation, and wherein pH and concentrations of hydroquinone and bromide ion are changed by the development process and wherein quantities of premixed replenishers are added to said bath to compensate for concentration changes due to development and to aging, the improvement comprising: replenishing said bath of lith developer solution to compensate for concentration changes due to development by repetitively adding to the developer solution as each quantity of film is developed, in combination: 1. a quantity of a stable solution concentrate A having a pH below 8 and consisting essentially of an aqueous solution of sufficient hydroquinone to replace that consumed during development of each quantity of film, 2. a quantity of stable solution concentrate B consisting essentially of a strongly basic aqueous solution having a pH above 9, and free of developing agent, the amount of concentrate B being sufficient to maintain the pH and constituent concentration of the developer; and wherein A, B, or A+B contains sodium formaldehyde bisulfite in an amount sufficient to act as a buffer for sulfite ion concentration.
Claim 3
Dependent Claim 15 words
The process of claim 1 wherein solution concentrate A, B, or A+B contains bromide ion.
Claim 4
Dependent Claim 20 words
The process of claim 1 wherein each solution concentrate is diluted with water as it is added to the developer.
Claim 5
Dependent Claim 23 words
The process of claim 1 wherein each solution concentrate is added directly to the developer, and water is separately added to the developer.
Claim 6
Dependent Claim 72 words
The process of claim 1 wherein a plurality of films are developed having differing bromide contents, and wherein solution concentrates A and B are substantially free of bromide ions, and wherein a third solution concentrate comprising aqueous bromide solution is added in combination with solution concentrates A and B to adjust commensurately for the bromide content of said film being developed so as to maintain the developer at a consistent bromide concentration.
Claim 7
Dependent Claim 22 words
The process of claim 5 wherein the third solution concentrate consists essentially of solution concentrate A or B with added bromide ion.
Claim 8
Dependent Claim 301 words
In a process of developing imagewise-exposed lithographic film in a bath of lith developer solution contained in an automatic photographic film processor, said solution containing hydroquinone as the sole developing agent and having a low sulfite ion concentration characterized by a high sensitivity to pH, to bromide ion, and to sulfite concentration changes, and being subject to aging due to aerial oxidation and anaerobic degradation, and in which pH and concentrations of hydroquinone and bromide ion are changed by the development process and quantities of premixed replenishers are added to said bath to compensate for concentration changes due to development and to aging, the improvement comprising: replenishing said lith developer solution to compensate for concentration changes due to development by repetitively adding to the developer solution as each quantity of film is developed, in combination: (1) a quantity of a stable solution concentrate A having a pH below 8 and consisting essentially of an aqueous solution of sufficient hydroquinone to replace that consumed during development of each quantity of film, (2) a quantity of stable solution concentrate B consisting essentially of a strongly basic aqueous solution having a pH above 9 and free of developing agent, the amount of concentrate B being sufficient to maintain the pH and constituent concentration of the developer; and wherein A, B, or A+B contains sodium formaldehyde bisulfite in an amount sufficient to act as a buffer for sulfite ion concentration, and replenishing to compensate for developer aging by repetitively adding to the developer at predetermined time intervals, in combination, a quantity of stable solution concentrate A and a quantity of stable solution concentrate C, the latter consisting essentially of solution concentrate B with increased bisulfite and bromide ion concentration; the amount of A and C added being sufficient to maintain original speed and dot quality.
Claim 9
Dependent Claim 301 words
In a process of developing imagewise-exposed lithographic film in a bath of lith developer solution contained in an automatic photographic film processor, said solution containing hydroquinone as the sole developing agent and having a low sulfite ion concentration characterized by a high sensitivity to pH, to bromide ion, and to sulfite concentration changes, and being subject to aging due to aerial oxidation and anaerobic degradation, and in which pH and concentrations of hydroquinone and bromide ion are changed by the development process and quantities of premixed replenishers are added to said bath to compensate for concentration changes due to development and to aging, the improvement comprising: replenishing said lith developer solution to compensate for concentration changes due to development by repetitively adding to the developer solution as each quantity of film is developed, in combination: (1) a quantity of a stable solution concentrate A having a pH below 8 and consisting essentially of an aqueous solution of sufficient hydroquinone to replace that consumed during development of each quantity of film, (2) a quantity of stable solution concentrate B consisting essentially of a strongly basic aqueous solution having a pH above 9 and free of developing agent, the amount of concentrate B being sufficient to maintain the pH and constituent concentration of the developer; and wherein A, B, or A+B contains sodium formaldehyde bisulfite in an amount sufficient to act as a buffer for sulfite ion concentration, and replenishing to compensate for developer aging by repetitively adding to the developer at predetermined time intervals, in combination, a quantity of stable solution concentrate A and a quantity of stable solution concentrate C, the latter consisting essentially of solution concentrate B with increased bisulfite and bromide ion concentration; the amount of A and C added being sufficient to maintain original speed and dot quality.
Claim 10
Dependent Claim 70 words
The process of claim 7 wherein concentrates A and C are added to the developer at regular time intervals in an amount equal to that which would be necessary to maintain a constant level of activity in the developer if no film were developed, minus the amount of replenisher A and B which was added during the previous time interval to compensate for consumption of developer due to film development.

References Cited (Backward Citations)

US2073664A Cited
US3334566A Cited
US3388653A Cited
US3472143A Cited
US3647462A Cited
DE2004893A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-05-23 1980-11-22 1981-05-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-05-23 1984-11-22 1985-05-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-05-23 1988-11-22 1989-05-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag