Homogeneous hydroxy-alkylation of cellulose

Assignee: Union Carbide Corp
•
Filing: 1976-05-04
•
Granted: 1977-05-17
•
Expires: 1996-05-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A solvent mixture consisting of dimethyl sulfoxide and formaldehyde is used for the hydroxy-alkylation of cellulose.

Inventors

  • 👤 Myron Donald Nicholson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 07:21
CPC Classifications
C; C08; C08B; C08B11/00; C08B11/02; C08B11/04; C08B11/08

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 59 words
The method of hydroxy-alkylating cellulose which comprises contacting a slurry of cellulose and dimethyl sulfoxide containing up to about 15 percent cellulose with sufficient formaldehyde to effect a homogeneous solution and then contacting said solution with a 1,2-alkylene oxide in the presence of a catalyst at a temperature of about 0° to 110° C. for at least one hour.
Claim 2
Independent Claim 59 words
The method of hydroxy-alkylating cellulose which comprises contacting a slurry of cellulose and dimethyl sulfoxide containing up to about 15 percent cellulose with sufficient formaldehyde to effect a homogeneous solution and then contacting said solution with a 1,2-alkylene oxide in the presence of a catalyst at a temperature of about 0° to 110° C. for at least one hour.
Claim 3
Dependent Claim 17 words
Method claimed in claim 1 wherein the concentration of cellulose in the homogeneous solution is about 15%.
Claim 4
Dependent Claim 12 words
Method claimed in claim 1 wherein the 1,2-alkylene oxide is ethylene oxide.
Claim 5
Dependent Claim 12 words
Method claimed in claim 1 wherein the 1,2-alkylene oxide is 1,2-propylene oxide.
Claim 6
Dependent Claim 12 words
Method claimed in claim 1 wherein the 1,2-alkylene oxide is 1,2-butylene oxide.
Claim 7
Dependent Claim 26 words
Method claimed in claim 1 wherein the 1,2-alkylene oxide is contacted with the homogeneous solution at a temperature of about 20° C. to about 60° C.

References Cited (Backward Citations)

US1234720A Cited
US1863208A Cited
US2679449A Cited
US3023183A Cited
US3278521A Cited
US3236669A Cited
US3644082A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-05-16 1980-11-15 1981-05-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-05-16 1984-11-15 1985-05-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-05-16 1988-11-15 1989-05-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag