Process for the manufacture of endless coated abrasive articles
Assignee: Saint Gobain Abrasives Inc
•
Filing: 1970-12-16
•
Granted: 1977-04-19
•
Expires: 1990-12-16
Abstract
Abstract An endless coated abrasive article is formed by helically winding a strip of abrasive material into a spiral of coils, the edges of which are in abutting engagement thus forming a spiral butt joint and coating the inner periphery of the helically wound strip of abrasive material with a continuous layer of resinous composition whereby an abrasive article is formed of greater width than the strip of abrasive material.
Inventors
- 👤 Hugh N. Dyer
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 13:05
CPC Classifications
B; B24; B24D; B24D11/00; B24D11/008
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
224 words
Process for the manufacture of an endless coated abrasive article comprising the following steps: a. cutting a coated abrasive material at a first location along the longitudinal edge at an angle to the length direction thereof such that the length of the cut edge is equal to the circumference of the article to be fabricated; b. cutting said material at a second location along said longitudinal edge and at a predetermined distance from said first location so as to provide a second cut edge parallel to said first cut edge thereby forming a strip of abrasive material having the shape of a parallelogram; c. winding said strip of abrasive into a spiral comprising a plurality of coils having the abrasive surface on the outside of said coils whereby said longitudinal edge is in abutting engagement with the other longitudinal edge of the parallelogram, said spiralled abrasive strip having an inner and outer periphery; d. rotating said spiralled abrasive strip about its own axis while said strip is rotating e. applying to said inner periphery smooth, uniformly thick, a resinous composition whereby said composition forms a continuous layer on the inner periphery of the coiled strip of abrasive material; and f. curing said resinous compositon thereby providing an endless coated abrasive article of unitary construction and of greater width than said strip of abrasive material.
Claim 2
Dependent Claim
224 words
Process for the manufacture of an endless coated abrasive article comprising the following steps: a. cutting a coated abrasive material at a first location along the longitudinal edge at an angle to the length direction thereof such that the length of the cut edge is equal to the circumference of the article to be fabricated; b. cutting said material at a second location along said longitudinal edge and at a predetermined distance from said first location so as to provide a second cut edge parallel to said first cut edge thereby forming a strip of abrasive material having the shape of a parallelogram; c. winding said strip of abrasive into a spiral comprising a plurality of coils having the abrasive surface on the outside of said coils whereby said longitudinal edge is in abutting engagement with the other longitudinal edge of the parallelogram, said spiralled abrasive strip having an inner and outer periphery; d. rotating said spiralled abrasive strip about its own axis while said strip is rotating e. applying to said inner periphery smooth, uniformly thick, a resinous composition whereby said composition forms a continuous layer on the inner periphery of the coiled strip of abrasive material; and f. curing said resinous compositon thereby providing an endless coated abrasive article of unitary construction and of greater width than said strip of abrasive material.
Claim 3
Dependent Claim
43 words
Process as in claim 1 wherein said resinous composition comprises, in addition to a suitable resin, a reinforcing material, said rotation being sufficient to cause a higher concentration of reinforcing material immediately adjacent the inner periphery of the coiled strip of abrasive material.
Claim 4
Dependent Claim
91 words
Process for the manufacture of an endless coated abrasive article comprising: a. positioning a strip of coated abrasive material having a grain side and a back side around the inner periphery of a circular-shaped mold, the back side of said strip material facing toward the mold center; b. introducing into the mold and onto said back side a resinous compositon having therein a fibrous reinforcing material; and c. rotating the mold during introduction of said composition so as to cast on the back side a uniform layer of the resin composition.
Claim 5
Dependent Claim
91 words
Process for the manufacture of an endless coated abrasive article comprising: a. positioning a strip of coated abrasive material having a grain side and a back side around the inner periphery of a circular-shaped mold, the back side of said strip material facing toward the mold center; b. introducing into the mold and onto said back side a resinous compositon having therein a fibrous reinforcing material; and c. rotating the mold during introduction of said composition so as to cast on the back side a uniform layer of the resin composition.
Claim 6
Dependent Claim
25 words
Process according to claim 3, wherein said coated abrasive strip material is parallelogram-shaped and such is helically wrapped around the inner periphery of said mold.
References Cited (Backward Citations)
US1788600A
Cited
US1929274A
Cited
US2219853A
Cited
US2106186A
Cited
US2534805A
Cited
US3014795A
Cited
US3037852A
Cited
US3402034A
Cited
US3413106A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-04-18 | 1980-10-18 | 1981-04-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-04-18 | 1984-10-18 | 1985-04-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-04-18 | 1988-10-18 | 1989-04-19 | $7700.00 | Window Closed / Lapsed |