Abstract

Abstract Wood and/or woody wastes, particularly coniferous woods, are treated to render them suitable as a high energy food for ruminating animals. Comminuted wood or woody wastes are impregnated with a glycol or glycol-ether solvent and a catalyst, and the mixture heated to a temperature of at least 145° C. for a time sufficient to delignify the wood the desired amount and solubilize extraneous components in the wood which are detrimental to the digestibility of the treated wood by the ruminant. The treated wood is then defibrated and the glycol solvent and catalyst extracted from the treated wood and recovered for recycle and reuse. The pulp recovered from extraction is a substantially anhydrous pulp which can be injected with nutrients promoting greater digestibility of the pulp and rehydrated for feeding to the ruminant.

Inventors

  • 👤 George O. Orth, Jr.
  • 👤 Richard D. Orth

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 14:15
CPC Classifications
D; D21; D21C; D21C3/00; D21C3/20; A; A23; A23K; A23K10/00; A23K10/30; A23K10/32; D21C3/22; D21C3/222; Y; Y10; Y10S; Y10S426/00; Y10S426/807

Claims Analysis

Total Claims: 18
Claim 1
Independent Claim 156 words
A method of making a food for ruminant animals which is substantially free from substances which are inimical to the microflora contained in the rumen of ruminant animals, comprising: comminuting wood and/or woody material impregnating the comminuted material with a solvent mixture consisting essentially of an acid catalyst and a glycol or glycol-ether solvent having from 2 to 6 carbon atoms, heating the material impregnated with the solvent mixture to a temperature of at least 145° C. for a time sufficient to delignify the wood at least 70% and solubilize the lignin and wood sugars contained in the material, subjecting the treated material to defibration to form a defibrated cellulose pulp, extracting the solvent mixture from the defibrated pulp with an extraction solvent containing a water-soluble, lower aliphatic alcohol having from 1 to 4 carbon atoms, recovering the solvent extracted pulp substantially in the anhydrous state, and rehydrating the substantially anhydrous pulp for feeding to ruminant
Claim 2
Independent Claim 156 words
A method of making a food for ruminant animals which is substantially free from substances which are inimical to the microflora contained in the rumen of ruminant animals, comprising: comminuting wood and/or woody material impregnating the comminuted material with a solvent mixture consisting essentially of an acid catalyst and a glycol or glycol-ether solvent having from 2 to 6 carbon atoms, heating the material impregnated with the solvent mixture to a temperature of at least 145° C. for a time sufficient to delignify the wood at least 70% and solubilize the lignin and wood sugars contained in the material, subjecting the treated material to defibration to form a defibrated cellulose pulp, extracting the solvent mixture from the defibrated pulp with an extraction solvent containing a water-soluble, lower aliphatic alcohol having from 1 to 4 carbon atoms, recovering the solvent extracted pulp substantially in the anhydrous state, and rehydrating the substantially anhydrous pulp for feeding to ruminant
Claim 3
Dependent Claim 53 words
The method of claim 1, including: subjecting the extraction solvent after the extraction step to distillation to recover the extraction solvent, leaving a distillation residue containing the solvent mixture, solubilized lignin, wood sugars and extraneous components, precipitating lignin from the distillation residue, and recovering the solvent mixture from the distillation residue for recycle
Claim 4
Dependent Claim 26 words
The method of claim 1 wherein the catalyst is hydrated aluminum chloride present in an amount ranging from 1-5% by weight based on the weight of
Claim 5
Dependent Claim 13 words
The method of claim 1 wherein the weight ratio of glycol solvent to
Claim 6
Dependent Claim 12 words
The method of claim 1 wherein the extraction solvent is an ethanol/water
Claim 7
Dependent Claim 22 words
The method of claim 1 wherein the glycol solvent is one selected from the group consisting ethylene glycol, diethylene glycol and triethylene
Claim 8
Dependent Claim 46 words
The method of claim 2 wherein solubilized lignin is precipitated from the distillation residue by mixing the distillation residue with water and heating the mixture to a temperature of about 70° C., the lignin precipitating from the solution in a form which is both filterable and
Claim 9
Dependent Claim 13 words
The method of claim 1 wherein extraction of the solvent mixture from the
Claim 10
Independent Claim 144 words
A method of making a food for ruminant animals from wood, the food substantially free from extraneous components and having a low lignin content comprising: comminuting the wood to be treated, impregnating the comminuted wood with a solvent mixture consisting essentially of triethylene glycol and an hydrated aluminum chloride catalyst, the catalyst present in an amount ranging from 1-5% by weight based on the weight of triethylene glycol, the weight ratio of solvent mixture to comminuted wood being at least 1.7:1, heating the wood impregnated with the solvent mixture to a temperature of at least 145° C. for a time ranging from 1 to 5 hours to delignify and solubilize the lignin, wood sugars and other extraneous components in the wood, subjecting the wood to defibration to form a cellulose pulp, extracting the solvent mixture from the pulp with an ethanol-containing extraction solvent, and
Claim 11
Independent Claim 144 words
A method of making a food for ruminant animals from wood, the food substantially free from extraneous components and having a low lignin content comprising: comminuting the wood to be treated, impregnating the comminuted wood with a solvent mixture consisting essentially of triethylene glycol and an hydrated aluminum chloride catalyst, the catalyst present in an amount ranging from 1-5% by weight based on the weight of triethylene glycol, the weight ratio of solvent mixture to comminuted wood being at least 1.7:1, heating the wood impregnated with the solvent mixture to a temperature of at least 145° C. for a time ranging from 1 to 5 hours to delignify and solubilize the lignin, wood sugars and other extraneous components in the wood, subjecting the wood to defibration to form a cellulose pulp, extracting the solvent mixture from the pulp with an ethanol-containing extraction solvent, and
Claim 12
Dependent Claim 11 words
The method of claim 9 wherein the extraction solvent is an
Claim 13
Dependent Claim 59 words
The method of claim 9, including: subjecting the extraction solvent containing triethylene glycol, catalyst, solubilized lignin, wood sugars and extraneous components to distillation to recover the extraction solvent, leaving a distillation residue containing triethylene glycol, catalyst, solubilized lignin, wood sugars and extraneous components, precipitating lignin from the distillation residue, and recovering triethylene glycol and its catalyst from the distillation
Claim 14
Dependent Claim 21 words
The method of claim 9 wherein extraction of the triethylene glycol and catalyst from the pulp is by continuous, multi-stage, countercurrent
Claim 15
Dependent Claim 12 words
The method of claim 9 wherein the impregnated wood is heated uniformly
Claim 16
Dependent Claim 40 words
The method of claim 9 wherein the comminuted wood is impregnated with the triethylene glycol/catalyst mixture by subjecting the wood to vacuum, introducing the triethylene glycol/catalyst mixture, and subjecting the wood/solvent mixture to pressure to uniformly impregnate the wood chips
Claim 17
Dependent Claim 25 words
The method of claim 9 including adding to the recovered pulp a nutrient useful to enhance the microflora in the digestion system of the ruminant,
Claim 18
Dependent Claim 16 words
The method of claim 9 including rehydrating the substantially anhydrous pulp for feeding to ruminant animals.

References Cited (Backward Citations)

US2003347A Cited
US2772968A Cited
US3069269A Cited
US3212933A Cited
US3502478A Cited
US3887426A Cited
US3796809A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-04-11 1980-10-11 1981-04-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-04-11 1984-10-11 1985-04-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-04-11 1988-10-11 1989-04-12 $7700.00 Window Closed / Lapsed