Abstract

Abstract Disclosed are the uses of polyphosphate solutions as fountain solutions in the dampener roll systems of offset presses and as rub-up solutions for preparing offset plates for storage without corrosion. In the fountain solution application of the invention, the polyphosphate concentration may run from about 0.6 g/l to about 42 g/l; in the plate storage application of the invention it may run from about 6 g/l to about 66 g/l. Particular polyphosphates which are useful in the invention include sodium tripolyphosphate, sodium hexametaphosphate and aminomethylenephosphonate.

Inventors

  • 👤 Dorvin Brown

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 21:49
CPC Classifications
B; B41; B41N; B41N3/00; B41N3/08

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 111 words
A method of offset printing with a metal printing plate of the kind which is susceptible to corrosion and which tends to accumulate dirt in the non-image regions thereof, comprising dampening the surface of said plate in the non-image regions thereof with an aqueous polyphosphate solution containing polyphosphate in an amount at least equal to about 0.6 g/l prior to inking said plate and taking an impression therefrom, in which the aqueous polyphosphate solution consists essentially of a concentrate consisting essentially of: ______________________________________ Volume Per Cent ______________________________________ Sodium tripolyphosphate 4.3 Sodium hexametaphosphate 21.5 Aminomethylenephosphonate 0.8 Water 73.4 ______________________________________ diluted to a use concentration between about 0.6 g/l and about 3 g/l.
Claim 2
Independent Claim 111 words
A method of offset printing with a metal printing plate of the kind which is susceptible to corrosion and which tends to accumulate dirt in the non-image regions thereof, comprising dampening the surface of said plate in the non-image regions thereof with an aqueous polyphosphate solution containing polyphosphate in an amount at least equal to about 0.6 g/l prior to inking said plate and taking an impression therefrom, in which the aqueous polyphosphate solution consists essentially of a concentrate consisting essentially of: ______________________________________ Volume Per Cent ______________________________________ Sodium tripolyphosphate 4.3 Sodium hexametaphosphate 21.5 Aminomethylenephosphonate 0.8 Water 73.4 ______________________________________ diluted to a use concentration between about 0.6 g/l and about 3 g/l.
Claim 3
Independent Claim 101 words
A method of offset printing with a metal printing plate of the kind which is susceptible to corrosion and which tends to accumulate dirt in the non-image regions thereof, comprising coating said plate with an aqueous polyphosphate solution containing polyphosphate in an amount between about 6 g/l and about 66 g/l, storing the coated plate until needed for use, and rinsing said stored coated plate after storage but prior to use, in which the aqueous polyphosphate solution consists essentially of a concentrate consisting essentially of: ______________________________________ Volume Per Cent ______________________________________ Sodium tripolyphosphate 4.3 Sodium hexametaphosphate 21.5 Aminomethylenephosphonate 0.8 Water 73.4 ______________________________________
Claim 4
Independent Claim 101 words
A method of offset printing with a metal printing plate of the kind which is susceptible to corrosion and which tends to accumulate dirt in the non-image regions thereof, comprising coating said plate with an aqueous polyphosphate solution containing polyphosphate in an amount between about 6 g/l and about 66 g/l, storing the coated plate until needed for use, and rinsing said stored coated plate after storage but prior to use, in which the aqueous polyphosphate solution consists essentially of a concentrate consisting essentially of: ______________________________________ Volume Per Cent ______________________________________ Sodium tripolyphosphate 4.3 Sodium hexametaphosphate 21.5 Aminomethylenephosphonate 0.8 Water 73.4 ______________________________________
Claim 5
Dependent Claim 30 words
A concentrate for use in fountain solutions and plate storage solutions consisting essentially of: ______________________________________ Volume Per Cent ______________________________________ Sodium tripolyphosphate 4.3 Sodium hexametaphosphate 21.5 Aminomethylenephosphonate 0.8 Water 73.4 ______________________________________
Claim 6
Dependent Claim 30 words
A concentrate for use in fountain solutions and plate storage solutions consisting essentially of: ______________________________________ Volume Per Cent ______________________________________ Sodium tripolyphosphate 4.3 Sodium hexametaphosphate 21.5 Aminomethylenephosphonate 0.8 Water 73.4 ______________________________________

References Cited (Backward Citations)

US2441653A Cited
US3354824A Cited
US3394653A Cited
US3696746A Cited
US3775135A Cited
US3764353A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-03-21 1980-09-20 1981-03-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-03-21 1984-09-20 1985-03-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-03-21 1988-09-20 1989-03-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag