Abstract A water-soluble composition capable of removing iron sulfide and sludge from metal surfaces and a method of such removal of iron sulfide and sludge from metal surfaces, particularly in a glycol system, the composition comprising: A. from about 2 to about 15% by weight of a high molecular weight linear diamine; B. from about 2.5 to about 18% by weight of acetic acid; C. from about 1 to about 10% by weight of an organic nitrogen substituted imidazoline; D. from about 6 to about 15% by weight of a non-ionic surfactant; E. from about 2 to about 8% by weight of a quaternary ammonium chloride; F. from about 1 to about 15% by weight of an alcohol solvent; and G. the remainder, water. In the method of removing iron sulfide and sludge from interior metal surfaces, particularly in a glycol system, the above composition is added to the effluent of the glycol system for onstream treatment in an amount effective to remove the iron sulfide and sludge. Generally, the composition is added to the effluent in an amount of from about 200 to about 1,000 parts per million of effluent.
A method of removing iron sulfide and sludge from interior metal surfaces in a glycol system which comprises introducing, onstream, into said glycol system an effective iron sulfide and sludge removing amount of a water and glycol soluble composition comprising: a. from about 2 to about 15% by weight of a high molecular weight diamine; b. from about 2.5 to about 18% by weight of acetic acid; c. from about 1 to about 10% by weight of an organic nitrogen substituted imidazoline of the formula; ##STR3## wherein R is an alkyl radical. d. from about 6 to about 15% by weight of a non-ionic surfactant; and e. from about 2 to about 8% by weight of a quaternary ammonium chloride. f. from about 1 to about 15% by weight of an alcohol solvent selected from the group consisting of diacetone alcohol and lower aliphatic alcohols; and g. the remainder, water.
Claim 2
Independent Claim
150 words
A method of removing iron sulfide and sludge from interior metal surfaces in a glycol system which comprises introducing, onstream, into said glycol system an effective iron sulfide and sludge removing amount of a water and glycol soluble composition comprising: a. from about 2 to about 15% by weight of a high molecular weight diamine; b. from about 2.5 to about 18% by weight of acetic acid; c. from about 1 to about 10% by weight of an organic nitrogen substituted imidazoline of the formula; ##STR3## wherein R is an alkyl radical. d. from about 6 to about 15% by weight of a non-ionic surfactant; and e. from about 2 to about 8% by weight of a quaternary ammonium chloride. f. from about 1 to about 15% by weight of an alcohol solvent selected from the group consisting of diacetone alcohol and lower aliphatic alcohols; and g. the remainder, water.
Claim 3
Dependent Claim
25 words
The method of claim 1, wherein said composition is introduced into the said glycol system in an amount of 200 to 1,000 parts per million.