Abstract

Abstract This invention relates to a process for the manufacture of graft copolymers based on methyl methacrylate polymers. The methyl methacrylate polymer is reacted with a high molecular weight organic compound containing at least one alkylene oxide unit having an alkali metal alcoholate end group, during which reaction transesterification occurs to eliminate alkali metal methoxide and cause chain joining. The graft copolymers may be used for the production of shaped articles or coating compositions and as additives, antistatic agents or adhesion promoters for plastics materials.

Inventors

  • 👤 Gerhard Fahrbach
  • 👤 Erhard Seiler
  • 👤 Dieter Stein

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 11:31
CPC Classifications
C; C08; C08G; C08G81/00; C08G81/02; C08G81/024; C08G81/025

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 87 words
A process for the manufacture of grafting living polyalkylene oxide on methyl methacrylate polymers, wherein a polymer of methyl methacrylate (A) containing at least 10% by weight of polymerized units of methyl methacrylate is reacted with a high molecular weight organic compound (B) consisting essentially of polyalkylene oxide with at least one alkylene oxide unit having an alkali metal alcoholate end group, said reaction being carried out in an anhydrous inert organic solvent by mixing solutions of components A and B at from -50° to +100° C.
Claim 2
Dependent Claim 87 words
A process for the manufacture of grafting living polyalkylene oxide on methyl methacrylate polymers, wherein a polymer of methyl methacrylate (A) containing at least 10% by weight of polymerized units of methyl methacrylate is reacted with a high molecular weight organic compound (B) consisting essentially of polyalkylene oxide with at least one alkylene oxide unit having an alkali metal alcoholate end group, said reaction being carried out in an anhydrous inert organic solvent by mixing solutions of components A and B at from -50° to +100° C.

References Cited (Backward Citations)

US3050511A Cited
US3175997A Cited
US3418354A Cited
US3499059A Cited
US3626027A Cited
US3786116A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-01-11 1980-07-12 1981-01-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-01-11 1984-07-12 1985-01-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-01-11 1988-07-12 1989-01-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag