Polymerizable organic dispersion of unsaturated polyester vinyl monomer and EVA copolymers

Assignee: Bayer AG
•
Filing: 1975-02-25
•
Granted: 1976-10-26
•
Expires: 1995-02-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Pourable and pumpable, storage-stable organic dispersions which can be cured with little shrinkage comprising unsaturated polyesters, copolymerizable vinyl monomers, ethylene vinyl ester copolymers and optionally dispersing agents.

Inventors

  • 👤 Heinrich Alberts
  • 👤 Hansjochen Schulz-Walz
  • 👤 Herbert Bartl
  • 👤 Leonhard Goerden
  • 👤 Klaus Schuster

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 07:09
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/02; C08J3/09; C08J5/00; C08J5/24; C08J5/241; C08J5/244; C08J5/249; C08L; C08L67/00; C08L67/06; C08J2367/00; C08J2367/06

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 106 words
A pourable and pumpable, storage-stable dispersion which can be cured with minimal shrinkage comprising 35-59% by weight of an unsaturated polyester, 40-64% by weight of a copolymerizable vinyl monomer, 1-20% by weight of a low shrinkage thermoplastic copolymer selected from the group consisting of ethylene/vinyl acetate copolymer, ethylene/vinyl propionate copolymer and mixtures thereof, each said copolymer containing 0.5-20% by weight of vinyl ester and said copolymer having up to 50% by weight thereof replaced by polyethylene, and 0.001-20% by weight of a dispersing agent which is an ethylene/vinyl acetate copolymer containing 60-99% by weight of vinyl acetate and having a Mooney viscosity of at least 15.
Claim 2
Dependent Claim 106 words
A pourable and pumpable, storage-stable dispersion which can be cured with minimal shrinkage comprising 35-59% by weight of an unsaturated polyester, 40-64% by weight of a copolymerizable vinyl monomer, 1-20% by weight of a low shrinkage thermoplastic copolymer selected from the group consisting of ethylene/vinyl acetate copolymer, ethylene/vinyl propionate copolymer and mixtures thereof, each said copolymer containing 0.5-20% by weight of vinyl ester and said copolymer having up to 50% by weight thereof replaced by polyethylene, and 0.001-20% by weight of a dispersing agent which is an ethylene/vinyl acetate copolymer containing 60-99% by weight of vinyl acetate and having a Mooney viscosity of at least 15.
Claim 3
Dependent Claim 73 words
A process for preparing a dispersion of claim 1 which comprises warming a solution of the unsaturated polyester in copolymerizable vinyl monomer and a solution of the low shrinkage thermoplastic copolymer to 50°-120° C., combining said warm solutions in the presence of said dispersing agent in a zone of high turbulence, withdrawing resulting mixture from said zone and stirring withdrawn mixture intensely at 50°-120° C. until a pourable state of low viscosity results.
Claim 4
Dependent Claim 18 words
A compression moulding material, injection moulding material or a resin mat prepared from a dispersion of claim 1.

References Cited (Backward Citations)

US3206441A Cited
US3331796A Cited
US3642683A Cited
US3718714A Cited
US3852376A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-10-26 1980-04-26 1980-10-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-10-26 1984-04-26 1984-10-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-10-26 1988-04-26 1988-10-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag