Abstract

Abstract Method for production of a zeolitic material represented by the formula: R.sub.x H.sub.5.sub.-x (Al.sub.y Fe.sub.1.sub.-y).sub.4 (P.sub.l As 1 -l ) 3 O 16 .zH 2 O wherein R represents Na or K, x, y, z and l are numerical values of O≦x≦5, O≦y≦1, Z≦9 and O≦l≦1, respectively; which comprises preparing an aqueous solution by dissolving (1) at least one source of aluminum and iron, (2) at least one source of phosphorus and arsenic and (3) at least one source of sodium and potassium in water in the ranges expressed in terms of the molar ratios of their oxides of 3.5≦(Al, Fe).sub. 2 O.sub.3 /(P, As).sub. 2 O.sub.5 ≦4.5 and (K, Na).sub.2 O/(Al, Fe) .sub.2 O.sub.3 >0.12 adjusting the pH of the solution to within the range of the cross-hatched area in FIGS. 1 to 4 and heating the solution at 150 to 250°C in a closed vessel to crystallize the zeolitic material and recovering the objective zeolitic material. The aforementioned zeolitic material is useful for recovering metallic cations from an aqueous solution containing such metallic cations.

Inventors

  • 👤 Takeo Wada
  • 👤 Kazuo Okada

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 12:53
CPC Classifications
C; C01; C01G; C01G28/00; C01G28/002; B; B01; B01J; B01J39/00; B01J39/02; C01B; C01B25/00; C01B25/16; C01B25/26; C01B25/45; C01P; C01P2002/00; C01P2002/70; C01P2002/72; C01P2002/77; C01P2006/00; C01P2006/80

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 256 words
A method for the production of a zeolitic material represented by the formula: R.sub.x H.sub.5.sub.-x (Al.sub.y Fe.sub.1.sub.-y).sub.4 (P.sub.l As.sub.1.sub.-l).sub.3 O.sub.16.zH.sub.2 O wherein R represents Na or K, x, y, z and l are numerical values of 0≦x≦5, 0≦y≦1, z≦9 and 0≦l≦1, respectively; which comprises preparing an aqueous solution by dissolving in water (1) at least one source of aluminum and iron selected from the group consisting of their chlorides, sulfides, nitrates, phosphates, arsenates, sulfates, acetates, oxides, hydroxides, gels soluble in alkalis or acids and alum containing either iron or aluminum, (2) at least one source of phosphorus and arsenic selected from the group consisting of phosphorus pentoxide, phosphoric acid, and condensed acids which give phosphoric acid when dissolved in water, sodium phosphate, potassium phosphate, ammonium phosphate, said phosphates including the mono- and di-hydrogen salts thereof, water-soluble calcium phosphate, strontium phosphate, aluminum phosphate, iron phosphate, arsenic pentoxide, arsenic acid, arsenous acid, sodium arsenate, potassium arsenate, ammonium arsenate, said arsenates including the mono- and di-hydrogen salts thereof, and (3) at least one source of sodium and potassium selected from the group consisting of their hydroxides, oxides and salts in the ranges expressed in terms of the molar ratios of their oxides of 3.5≦(Al, Fe).sub.2 O.sub.3 /(P, As).sub.2 O.sub.5 ≦4.5 and (K, Na).sub.2 O/(Al, Fe).sub.2 O.sub.3 >0.12 adjusting the pH of the solution to within the range of the cross-hatched area in FIGS. 1 to 4 and heating the solution at 150° to 250°C in a closed vessel to crystallize the zeolitic material and recovering the objective zeolitic material.
Claim 2
Independent Claim 256 words
A method for the production of a zeolitic material represented by the formula: R.sub.x H.sub.5.sub.-x (Al.sub.y Fe.sub.1.sub.-y).sub.4 (P.sub.l As.sub.1.sub.-l).sub.3 O.sub.16.zH.sub.2 O wherein R represents Na or K, x, y, z and l are numerical values of 0≦x≦5, 0≦y≦1, z≦9 and 0≦l≦1, respectively; which comprises preparing an aqueous solution by dissolving in water (1) at least one source of aluminum and iron selected from the group consisting of their chlorides, sulfides, nitrates, phosphates, arsenates, sulfates, acetates, oxides, hydroxides, gels soluble in alkalis or acids and alum containing either iron or aluminum, (2) at least one source of phosphorus and arsenic selected from the group consisting of phosphorus pentoxide, phosphoric acid, and condensed acids which give phosphoric acid when dissolved in water, sodium phosphate, potassium phosphate, ammonium phosphate, said phosphates including the mono- and di-hydrogen salts thereof, water-soluble calcium phosphate, strontium phosphate, aluminum phosphate, iron phosphate, arsenic pentoxide, arsenic acid, arsenous acid, sodium arsenate, potassium arsenate, ammonium arsenate, said arsenates including the mono- and di-hydrogen salts thereof, and (3) at least one source of sodium and potassium selected from the group consisting of their hydroxides, oxides and salts in the ranges expressed in terms of the molar ratios of their oxides of 3.5≦(Al, Fe).sub.2 O.sub.3 /(P, As).sub.2 O.sub.5 ≦4.5 and (K, Na).sub.2 O/(Al, Fe).sub.2 O.sub.3 >0.12 adjusting the pH of the solution to within the range of the cross-hatched area in FIGS. 1 to 4 and heating the solution at 150° to 250°C in a closed vessel to crystallize the zeolitic material and recovering the objective zeolitic material.
Claim 3
Dependent Claim 104 words
A method as claimed in claim 1, wherein x, y, and l have numerical values of 0<x<5, 0<y≦1 and 0<l≦1, respectively, and the aqueous solution is prepared by dissolving (1) at least one source of aluminum or a mixture of at least one source of aluminum and at least one source of iron, (2) at least one source of phosphorus or a mixture of at least one source of phosphorus and at least one source of arsenic and (3) at least one source of sodium and potassium in water wherein the sources of components (1), (2) and (3) are as defined in claim 1.
Claim 4
Dependent Claim 81 words
A method as claimed in claim 1, wherein y and l have numerical values of 0<y<1 and 0<l<1, respectively, and the aqueous solution is prepared by dissolving (1) at least one source of aluminum, (2) at least one source of iron, (3) at least one source of phosphorus, (4) at least one source of arsenic and (5) at least one source of sodium and potassium in water wherein the sources of components (1) to (5) are as defined in claim 1.
Claim 5
Dependent Claim 114 words
A method as claimed in claim 1, wherein y and l have numerical values of 1 and 1, respectively, and the aqueous solution is prepared by dissolving (1) at least one source of aluminum, (2) at least one source of phosphorus and (3) at least one source of sodium and potassium in water in the ranges expressed in terms of the molar ratios of their oxides of 3.5≦Al.sub.2 O.sub.3 /P.sub.2 O.sub.5 ≦4.5 and (K, Na).sub.2 O/Al.sub.2 O.sub.3 >0.12 and the pH of the solution is adjusted to within the range of the cross-hatched area in FIGS. 1 and 3 and wherein the sources of components (1) to (3) are as defined in claim 1.
Claim 6
Dependent Claim 111 words
A method as claimed in claim 1, wherein y and l are numerical numbers of 0<y<1 and 1, respectively, and the aqueous solution is prepared by dissolving (1) at least one source of aluminum, (2) at least one source of iron, (3) at least one source of phosphorus and (4) at least one source of sodium and potassium in water in the ranges of 3.5≦(Al, Fe).sub.2 O.sub.3 /P.sub.2 O.sub.5 ≦4.5 and (K, Na).sub.2 O/(Al, Fe).sub.2 O.sub.3 >0.12 and the pH of the solution is adjusted to within the range of the cross-hatched area in FIG. 1 and wherein the sources of components (1) to (4) are as defined in claim 1.
Claim 7
Dependent Claim 109 words
A method as claimed in claim 1, wherein y and l are numerical values of 1 and 0<l<1, respectively, and the aqueous solution is prepared by dissolving (1) at least one source of aluminum, (2) at least one source of phosphorus, (3) at least one source of arsenic and (4) at least one source of sodium and potassium in water in the ranges of 3.5≦Al.sub.2 O.sub.3 /P, As).sub.2 O.sub.5 ≦4.5 and (K,Na).sub.2 O/Al.sub.2 O.sub.3 >0.12 and the pH of the solution is adjusted to within the range of the cross-hatched area in FIG. 3 and wherein the sources of components (1) to (4) are as defined in claim 1.

References Cited (Backward Citations)

US3056647A Cited
US3311448A Cited
US3418072A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-09-21 1980-03-22 1980-09-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-09-21 1984-03-22 1984-09-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-09-21 1988-03-22 1988-09-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag