Abstract
Abstract The aging and thermal hysteresis of quartz crystal resonators are reduced hermetically sealing the quartz crystal resonator in a housng including a material transparent to radiation capable of polymerizing contaminants, and irradiating the resonator with radiation capable of polymerizing contaminants.
Inventors
- 👤 John R. Vig
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 21:59
CPC Classifications
H; H03; H03H; H03H3/00; H03H3/007; H03H3/02; H03H3/04; H10; H10N; H10N30/00; H10N30/01; H10N30/04; Y; Y10; Y10T; Y10T29/00; Y10T29/42
Claims Analysis
Total Claims: 16
Claim 1
Independent Claim
56 words
A method of reducing the aging and thermal hysteresis of quartz crystal resonators, said method including the steps of: a. hermetically sealing the quartz crystal resonator in a housing including a material transparent to ultraviolet radiation capable of polymerizing contaminants, and b. irradiating the contaminants within said resonator housing with ultraviolet radiation to polymerize said contaminants.
Claim 2
Independent Claim
56 words
A method of reducing the aging and thermal hysteresis of quartz crystal resonators, said method including the steps of: a. hermetically sealing the quartz crystal resonator in a housing including a material transparent to ultraviolet radiation capable of polymerizing contaminants, and b. irradiating the contaminants within said resonator housing with ultraviolet radiation to polymerize said contaminants.
Claim 3
Dependent Claim
16 words
Method according to claim 1 wherein the resonator is hermetically sealed in an oxygen free environment.
Claim 4
Dependent Claim
36 words
Method according to claim 1 wherein said housing material transparent to radiation capable of polymerizing contaminants is selected from the group consisting of fused quartz, sapphire, lithium fluoride, calcium fluoride, magnesium fluoride, and high silica glass.
Claim 5
Dependent Claim
12 words
Method according to claim 3 wherein said housing material is fused quartz.
Claim 6
Dependent Claim
11 words
Method according to claim 3 wherein said housing material is sapphire.
Claim 7
Dependent Claim
12 words
Method according to claim 3 wherein said housing material is lithium fluoride.
Claim 8
Dependent Claim
12 words
Method according to claim 3 wherein said housing material is calcium fluoride.
Claim 9
Dependent Claim
12 words
Method according to claim 3 wherein said housing material is magnesium fluoride.
Claim 10
Dependent Claim
13 words
Method according to claim 3 wherein said housing material is high silica glass.
Claim 11
Dependent Claim
68 words
Method according to claim 1 wherein said housing material transparent to radiation capable of polymerizing contaminants is selected from the group consisting of fused quartz, sapphire, lithium fluoride, calcium fluoride, magnesium fluoride and high silica glass, and wherein said quartz crystal resonator is irradiated from a radiation source capable of polymerizing contaminants and selected from the group consisting of ultraviolet, electron beam, gamma rays, glow discharge, and X-rays.
Claim 12
Dependent Claim
26 words
Method according to claim 10 wherein said housing material transparent to radiation capable of polyerizing contaminants is fused quartz and wherein said radiation source is ultraviolet.
Claim 13
Dependent Claim
20 words
Method according to claim 1 wherein the radiation is directed to areas other than the active area of the resonator.
Claim 14
Dependent Claim
14 words
Method according to claim 1 wherein the quartz crystal resonator is cooled during irradiation.
Claim 15
Dependent Claim
132 words
Method of reducing the aging and thermal hysteresis of quartz crystal resonators, said method consisting of enclosing the quartz crystal resonator in a housing including a ceramic frame with fused quartz top and bottom lids, hermetically sealing the resonator within the housing in an oxygen free environment and irradiating the mounted quartz crystal resonator for 5 minutes with ultraviolet radiation from an ultraviolet lamp at a distance of about 1 centimeter from the resonator so that both sides of the resonator are exposed to ultraviolet radiation, and wherein the ultraviolet lamp used is a low pressure mercury lamp in a fused quartz envelope with an intensity at 2 centimeters from the source of 2 milliwatts per centimeter squared of radiation at 2537A and 0.1 milliwatt per centimeter squared of radiation at 1849A.
Claim 16
Dependent Claim
132 words
Method of reducing the aging and thermal hysteresis of quartz crystal resonators, said method consisting of enclosing the quartz crystal resonator in a housing including a ceramic frame with fused quartz top and bottom lids, hermetically sealing the resonator within the housing in an oxygen free environment and irradiating the mounted quartz crystal resonator for 5 minutes with ultraviolet radiation from an ultraviolet lamp at a distance of about 1 centimeter from the resonator so that both sides of the resonator are exposed to ultraviolet radiation, and wherein the ultraviolet lamp used is a low pressure mercury lamp in a fused quartz envelope with an intensity at 2 centimeters from the source of 2 milliwatts per centimeter squared of radiation at 2537A and 0.1 milliwatt per centimeter squared of radiation at 1849A.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1979-09-21 | 1980-03-22 | 1980-09-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1983-09-21 | 1984-03-22 | 1984-09-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1987-09-21 | 1988-03-22 | 1988-09-21 | $7700.00 | Window Closed / Lapsed |