Abstract

Abstract A resin-coated high pressure glass bottle prepared by forming a first layer with pullulan on the exterior surface of a high pressure glass bottle and then overcoating this first layer with a resin of high alkali resistance, e.g. an epoxy, urethane or ethyl cellulose resin.

Inventors

  • 👤 Atsuo Mori
  • 👤 Kozo Tsuji
  • 👤 Shuji Kitamura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 20:14
CPC Classifications
C; C08; C08L; C08L5/00; B; B65; B65D; B65D23/00; B65D23/08; B65D23/0807; B65D23/0814; C03; C03C; C03C17/00; C03C17/28; C03C17/32; C03C17/34; C03C17/3405; Y; Y02; Y02P; Y02P20/00; Y02P20/50; Y02P20/582; Y10; Y10T; Y10T428/00; Y10T428/13; Y10T428/131; Y10T428/1317; Y10T428/1321; Y10T428/26; Y10T428/31504; Y10T428/31511; Y10T428/31551

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 70 words
A resin-coated glass bottle which comprises a pullulan resin coating layer on the exterior surface of a bottle, and an alkali resistant resin coating layer on said pullulan resin coating layer, wherein the thickness of the pullulan resin coating layer is 100 to 1,000μ, wherein the thickness of the alkali-resistant resin coating layer is 10 to 500μ and wherein the molecular weight of the pullulan resin is 50,000 to 3,500,000.
Claim 2
Dependent Claim 70 words
A resin-coated glass bottle which comprises a pullulan resin coating layer on the exterior surface of a bottle, and an alkali resistant resin coating layer on said pullulan resin coating layer, wherein the thickness of the pullulan resin coating layer is 100 to 1,000μ, wherein the thickness of the alkali-resistant resin coating layer is 10 to 500μ and wherein the molecular weight of the pullulan resin is 50,000 to 3,500,000.
Claim 3
Dependent Claim 20 words
A resin-coated glass bottle according to claim 1, wherein the alkali-resistant resin is an epoxy, urethane or ethyl cellulose resin.
Claim 4
Dependent Claim 16 words
A resin-coated glass bottle according to claim 1, wherein the alkali-resistant resin is an urethane resin.

References Cited (Backward Citations)

US3784390A Cited
US3823032A Cited
US3870537A Cited
US3888809A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-08-24 1980-02-23 1980-08-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-08-24 1984-02-23 1984-08-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-08-24 1988-02-23 1988-08-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags