Abstract

Abstract An electrode structure comprising a tube of substantially electrically insulating material such as glass, having a rounded tip of substantially electrically insulating material such as rubber, which tip has a capillary opening therethrough, encloses a metallic cathode and liquid electrolyte, and that electrode structure is placed with the tip and capillary opening in contact with the surface of a sample conductive substrate having an electrical barrier layer thereon whose thickness is to be measured, and electrical potential is applied between the cathode and sample conductive substrate, which is the anode in the system, and the thickness of the electrical barrier layer is measured as a function of the highest applied voltage that does not produce a pronounced increase in current flow in the system.

Inventors

  • 👤 Dominic J. Angelini
  • 👤 Philip G. Perry

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 15:24
CPC Classifications
G; G01; G01B; G01B7/00; G01B7/02; G01B7/06

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 124 words
An electrode structure consisting essentially of: a hollow tube of substantially electrically insulating material; a tip portion of substantially electrically insulating material closing one end of said tube, with a capillary orifice with a diameter less than about 1/16 of an inch extending through the thickness of said tip portion; a piece of electrode material extending into said tube from the end opposite said tip portion; an electrolyte which is nondestructive to a layer the thickness of which is to be measured and selected from the group consisting of tartaric acid, isopropyl alcohol, sodium formate, sodium chloride, potassium iodide, other halides of light metals and mixtures thereof within said tube and said tip portion, with the piece of electrode material extending into said electrolyte.
Claim 2
Dependent Claim 124 words
An electrode structure consisting essentially of: a hollow tube of substantially electrically insulating material; a tip portion of substantially electrically insulating material closing one end of said tube, with a capillary orifice with a diameter less than about 1/16 of an inch extending through the thickness of said tip portion; a piece of electrode material extending into said tube from the end opposite said tip portion; an electrolyte which is nondestructive to a layer the thickness of which is to be measured and selected from the group consisting of tartaric acid, isopropyl alcohol, sodium formate, sodium chloride, potassium iodide, other halides of light metals and mixtures thereof within said tube and said tip portion, with the piece of electrode material extending into said electrolyte.
Claim 3
Dependent Claim 23 words
The electrode structure of claim 1 wherein said capillary orifice is of a diameter of not greater than about 1/64 of an inch.
Claim 4
Dependent Claim 21 words
The electrode structure of claim 1, wherein said tube comprises relatively rigid material, and said tip portion comprises relatively flexible material.
Claim 5
Dependent Claim 13 words
The electrode structure of claim 3, wherein said tip portion comprises silicone rubber.
Claim 6
Dependent Claim 12 words
The electrode structure of claim 1, wherein said electrode material comprises aluminum.
Claim 7
Dependent Claim 12 words
The electrode structure of claim 1, wherein said electrode material comprises platinum.
Claim 8
Dependent Claim 34 words
The electrode structure of claim 1, wherein said electrode material comprises a material selected from the group consisting of: nickel, chromium, silver, copper, steel, gold, palladium or other Group VIII metals, carbon, or graphite.
Claim 9
Dependent Claim 24 words
The electrode structure of claim 1, wherein the electrolyte comprises a liquid having a pH in the range of about 2 to about 12.
Claim 10
Dependent Claim 24 words
The electrode structure of claim 5, wherein the electrolyte comprises a liquid having a pH in the range of about 5.0 to about 9.0.
Claim 11
Dependent Claim 246 words
Apparatus for measuring the thickness of an electrical barrier layer on a conductive substrate, consisting essentially of: providing an electrode structure consisting essentially of: a hollow tube of substantially electrically insulating material; a tip portion of substantially electrically insulating material closing one end of said tube, with a capillary orifice of a diameter less than about 1/16 of an inch extending through the thickness of said tip portion; a piece of electrode material extending into said tube from the end opposite said tip portion; an electrolyte which is nondestructive to a layer the thickness of which is to be measured and selected from the group consisting of tartaric acid, isopropyl alcohol, sodium formate, sodium chloride, potassium iodide, other halides of light metals, and mixtures thereof within said tube and said tip portion, with the piece of electrode material extending into said electrolyte; a DC power supply, including means for increasing voltage per unit time, the negative pole of said supply being electrically connected to the piece of electrode material of said electrode structure, and means connected to the positive pole of said power supply for contacting a sample conductive substrate; a voltmeter circuit connected for measuring the voltage provided to said electrode structure; an ammeter circuit connected for measuring the current flow through said electrode structure; an X-Y recorder connected to the output of said voltmeter circuit and to the output of said ammeter circuit for simultaneously recording said current as a function of said voltage.
Claim 12
Dependent Claim 246 words
Apparatus for measuring the thickness of an electrical barrier layer on a conductive substrate, consisting essentially of: providing an electrode structure consisting essentially of: a hollow tube of substantially electrically insulating material; a tip portion of substantially electrically insulating material closing one end of said tube, with a capillary orifice of a diameter less than about 1/16 of an inch extending through the thickness of said tip portion; a piece of electrode material extending into said tube from the end opposite said tip portion; an electrolyte which is nondestructive to a layer the thickness of which is to be measured and selected from the group consisting of tartaric acid, isopropyl alcohol, sodium formate, sodium chloride, potassium iodide, other halides of light metals, and mixtures thereof within said tube and said tip portion, with the piece of electrode material extending into said electrolyte; a DC power supply, including means for increasing voltage per unit time, the negative pole of said supply being electrically connected to the piece of electrode material of said electrode structure, and means connected to the positive pole of said power supply for contacting a sample conductive substrate; a voltmeter circuit connected for measuring the voltage provided to said electrode structure; an ammeter circuit connected for measuring the current flow through said electrode structure; an X-Y recorder connected to the output of said voltmeter circuit and to the output of said ammeter circuit for simultaneously recording said current as a function of said voltage.
Claim 13
Dependent Claim 22 words
The apparatus of claim 10, additionally comprising a sample conductive substrate in electrical contact with said means for contacting such a sample.
Claim 14
Dependent Claim 54 words
The apparatus of claim 11, wherein the tip portion of the electrode structure is in contact with the surfaces of said sample upon which there is a barrier layer whose thickness is to be measured, and the electrolyte is in electrical contact with said barrier layer through the capillary orifice in said tip portion.
Claim 15
Dependent Claim 24 words
The apparatus of claim 12, wherein the piece of electrode material in the electrode structure, and the sample conductive substrate, comprise the same material.
Claim 16
Dependent Claim 37 words
The apparatus of claim 10, wherein said piece of electrode material is a material selected from the group consisting of: aluminum, platinum, nickel, chromium, silver, copper, steel, gold, palladium or other Group VIII metals, carbon or graphite.
Claim 17
Independent Claim 283 words
A method of measuring the thickness of an electrical barrier layer on a conductive substrate, consisting essentially of: providing an electrode structure consisting essentially of: a hollow tube of substantially electrically insulating material; a tip portion of substantially electrically insulating material closing one end of said tube, with a capillary orifice of a diameter less than about 1/16 of an inch extending through the thickness of said tip portion; a piece of electrode material extending into said tube from the end opposite said tip portion; an electrolyte which is nondestructive to a layer the thickness of which is to be measured and selected from the group consisting of tartaric acid, isopropyl alcohol, sodium formate, sodium chloride, potassium iodide, other halides of light metals, and mixtures thereof within said tube and said tip portion, with the piece of electrode material extending into said electrolyte; placing the tip portion of the electrode structure in contact with the surface of a sample conductive substrate upon which there is a barrier layer whose thickness is to be measured, so that there is electrical contact between the electrolyte in said electrode structure and said barrier layer, through the capillary orifice in the tip portion of said electrode structure; connecting the electrode material of said electrode structure to the negative terminal of a DC power supply and connecting the conductive substrate to the positive terminal of said DC power supply; increasing the voltage from zero incrementally per unit time and simultaneously measuring said voltage and the current through said electrode structure, for thereby determining the highest voltage that does not produce a pronounced increase in current flow, which highest voltage is proportional to the thickness of said barrier layer.
Claim 18
Independent Claim 283 words
A method of measuring the thickness of an electrical barrier layer on a conductive substrate, consisting essentially of: providing an electrode structure consisting essentially of: a hollow tube of substantially electrically insulating material; a tip portion of substantially electrically insulating material closing one end of said tube, with a capillary orifice of a diameter less than about 1/16 of an inch extending through the thickness of said tip portion; a piece of electrode material extending into said tube from the end opposite said tip portion; an electrolyte which is nondestructive to a layer the thickness of which is to be measured and selected from the group consisting of tartaric acid, isopropyl alcohol, sodium formate, sodium chloride, potassium iodide, other halides of light metals, and mixtures thereof within said tube and said tip portion, with the piece of electrode material extending into said electrolyte; placing the tip portion of the electrode structure in contact with the surface of a sample conductive substrate upon which there is a barrier layer whose thickness is to be measured, so that there is electrical contact between the electrolyte in said electrode structure and said barrier layer, through the capillary orifice in the tip portion of said electrode structure; connecting the electrode material of said electrode structure to the negative terminal of a DC power supply and connecting the conductive substrate to the positive terminal of said DC power supply; increasing the voltage from zero incrementally per unit time and simultaneously measuring said voltage and the current through said electrode structure, for thereby determining the highest voltage that does not produce a pronounced increase in current flow, which highest voltage is proportional to the thickness of said barrier layer.
Claim 19
Dependent Claim 23 words
The method of claim 15, wherein said voltage and current are simultaneously measured and plotted in graphic form by an X-Y recording device.

References Cited (Backward Citations)

US2345498A Cited
US2497052A Cited
US2894882A Cited
US3315270A Cited
US3445366A Cited
US3293155A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-08-17 1980-02-16 1980-08-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-08-17 1984-02-16 1984-08-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-08-17 1988-02-16 1988-08-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag