Abstract

Abstract An information is written or erased in such way that, while a memory employing electrooptic ceramics wherein a ferroelectric phase and an anti-ferroelectric phase (or paraelectric phase) coexist having a morphotropic phase boundary is being heated to a temperature at which the polymorphic base boundary of the ceramic material occurs, an electric field opposite in polarity to the spontaneous polarization of the memory is applied to the material.

Inventors

  • 👤 Akio Kumada
  • 👤 Koji Ishida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 22:47
CPC Classifications
H; H01; H01G; H01G7/00; H01G7/02; H01G7/025; H01G7/026; C; C04; C04B; C04B35/00; C04B35/01; C04B35/46; C04B35/48; C04B35/50; C04B35/51; G; G02; G02F; G02F1/00; G02F1/01; G02F1/03; G02F1/055; G11; G11C; G11C11/00; G11C11/21; G11C11/22; G11C13/00; G11C13/04; G11C13/047

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 234 words
A method for erasing information stored in an electrooptic ceramic plate composed of an electrooptic ceramic in which a ferroelectric phase and an anti-ferroelectric or para-electric phase can coexist with a morphotropic phase boundary therebetween, said electrooptic ceramic formed from a solid solution of the following formula ##EQU2## wherein A denotes at least one element selected from the group consisting of Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Sb, Bi, La, Ce, Nd, Sm, Eu, Gd, Tb, and Dy, M representing at least one element selected from the group consisting of Fe, Ni, Co, Hf, Si, Ge, Sn, V, Nb, and Ta, said information being stored in the form of a pattern in said electrooptic ceramic plate, said pattern being defined by regions in the ferroelectric phase and regions in the anti-ferroelectric or para-electric phase, said method comprising a. maintaining said electrooptic ceramic plate at a temperature intermediate the temperature T(h) generating the heating morphotropic phase boundary in said electrooptic ceramic and the temperature T(c) generating the limiting morphotropic phase boundary in said electrooptic ceramic, and b. applying an electric field reverse in polarity to the spontaneous polarization of the ferroelectric phase in said electrooptic ceramic plate and simultaneously heating said electrooptic ceramic plate by the current of said applied electric field to a temperature higher than the temperature T(h), whereby the stored information is erased from said electrooptic ceramic plate.
Claim 2
Independent Claim 234 words
A method for erasing information stored in an electrooptic ceramic plate composed of an electrooptic ceramic in which a ferroelectric phase and an anti-ferroelectric or para-electric phase can coexist with a morphotropic phase boundary therebetween, said electrooptic ceramic formed from a solid solution of the following formula ##EQU2## wherein A denotes at least one element selected from the group consisting of Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Sb, Bi, La, Ce, Nd, Sm, Eu, Gd, Tb, and Dy, M representing at least one element selected from the group consisting of Fe, Ni, Co, Hf, Si, Ge, Sn, V, Nb, and Ta, said information being stored in the form of a pattern in said electrooptic ceramic plate, said pattern being defined by regions in the ferroelectric phase and regions in the anti-ferroelectric or para-electric phase, said method comprising a. maintaining said electrooptic ceramic plate at a temperature intermediate the temperature T(h) generating the heating morphotropic phase boundary in said electrooptic ceramic and the temperature T(c) generating the limiting morphotropic phase boundary in said electrooptic ceramic, and b. applying an electric field reverse in polarity to the spontaneous polarization of the ferroelectric phase in said electrooptic ceramic plate and simultaneously heating said electrooptic ceramic plate by the current of said applied electric field to a temperature higher than the temperature T(h), whereby the stored information is erased from said electrooptic ceramic plate.
Claim 3
Independent Claim 222 words
A method for writing information in an electrooptic ceramic plate composed of an electrooptic ceramic in which a ferroelectric and anti-ferroelectric or para-electric phase can coexist with a morphotropic phase boundary therebetween, said electrooptic ceramic formed from a solid solution of the following formula ##EQU3##wherein A denotes at least one element selected from the group consisting of Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Sb, Bi, La, Ce, Nd, Sm, Eu, Gd, Tb, and Dy, M representing at least one element selected from the group consisting of Fe, Ni, Co, Hf, Si, Ge, Sn, J, Nb, and Ta, said electrooptic ceramic plate being entirely in the ferroelectric state, said electrooptic ceramic being maintained at a temperature intermediate the temperature T(h) generating the heating morphotropic phase boundary in said electrooptic ceramic and the temperature T(c) generating the limiting morphotropic phase boundary in said electrooptic ceramic, said method comprising applying to said electrooptic plate an electric field reverse in polarity to the spontaneous polarization of said electrooptic ceramic plate in accordance with the pattern of the desired information to be written into said electrooptic ceramic plate and simultaneously heating said electrooptic ceramic plate in accordance with said pattern by the current produced by said electric field to a temperature above T(h) to thereby write said information into said electrooptic ceramic plate.
Claim 4
Independent Claim 222 words
A method for writing information in an electrooptic ceramic plate composed of an electrooptic ceramic in which a ferroelectric and anti-ferroelectric or para-electric phase can coexist with a morphotropic phase boundary therebetween, said electrooptic ceramic formed from a solid solution of the following formula ##EQU3##wherein A denotes at least one element selected from the group consisting of Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Sb, Bi, La, Ce, Nd, Sm, Eu, Gd, Tb, and Dy, M representing at least one element selected from the group consisting of Fe, Ni, Co, Hf, Si, Ge, Sn, J, Nb, and Ta, said electrooptic ceramic plate being entirely in the ferroelectric state, said electrooptic ceramic being maintained at a temperature intermediate the temperature T(h) generating the heating morphotropic phase boundary in said electrooptic ceramic and the temperature T(c) generating the limiting morphotropic phase boundary in said electrooptic ceramic, said method comprising applying to said electrooptic plate an electric field reverse in polarity to the spontaneous polarization of said electrooptic ceramic plate in accordance with the pattern of the desired information to be written into said electrooptic ceramic plate and simultaneously heating said electrooptic ceramic plate in accordance with said pattern by the current produced by said electric field to a temperature above T(h) to thereby write said information into said electrooptic ceramic plate.
Claim 5
Independent Claim 242 words
A method for writing information in an electrooptic ceramic plate composed of an electrooptic ceramic in which a ferroelectric and anti-ferroelectric or para-electric phase can coexist with a morphotrophic phase boundary therebetween, said electrooptic ceramic formed from a solid solution of the following formula: ##EQU4## wherein A denotes at least one element selected from the group consisting of Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Sb, Bi, La, Ce, Nd, Sm, Eu, Gd, Tb, and Dy, M representing at least one element selected from the group consisting of Fe, Ni, Co, Hf, Si, Ge, Sn, J, Nb, and Ta, said method comprising a. maintaining said electrooptic ceramic plate at a temperature intermediate the temperature T(h) generating the heating morphotropic phase boundary in said electrooptic ceramic and the temperature T(c) generating the limiting morphotropic phase boundary in said electrooptic ceramic, b. applying an electric field to said electrooptic ceramic plate to thereby change the state of said plate entirely to ferroelectric state and then c. applying to said electrooptic ceramic plate an electric field reverse in polarity to the spontaneous polarization of said electrooptic ceramic plate in accordance with the pattern of the desired information signal to be written into said electrooptic ceramic plate and simultaneously heating said electrooptic ceramic plate in accordance with said pattern by the current produced by said electric field to a temperature above temperature T(h) to thereby write said information into said electrooptic ceramic plate.
Claim 6
Independent Claim 242 words
A method for writing information in an electrooptic ceramic plate composed of an electrooptic ceramic in which a ferroelectric and anti-ferroelectric or para-electric phase can coexist with a morphotrophic phase boundary therebetween, said electrooptic ceramic formed from a solid solution of the following formula: ##EQU4## wherein A denotes at least one element selected from the group consisting of Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Sb, Bi, La, Ce, Nd, Sm, Eu, Gd, Tb, and Dy, M representing at least one element selected from the group consisting of Fe, Ni, Co, Hf, Si, Ge, Sn, J, Nb, and Ta, said method comprising a. maintaining said electrooptic ceramic plate at a temperature intermediate the temperature T(h) generating the heating morphotropic phase boundary in said electrooptic ceramic and the temperature T(c) generating the limiting morphotropic phase boundary in said electrooptic ceramic, b. applying an electric field to said electrooptic ceramic plate to thereby change the state of said plate entirely to ferroelectric state and then c. applying to said electrooptic ceramic plate an electric field reverse in polarity to the spontaneous polarization of said electrooptic ceramic plate in accordance with the pattern of the desired information signal to be written into said electrooptic ceramic plate and simultaneously heating said electrooptic ceramic plate in accordance with said pattern by the current produced by said electric field to a temperature above temperature T(h) to thereby write said information into said electrooptic ceramic plate.

References Cited (Backward Citations)

US3710352A Cited
US3871745A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-08-03 1980-02-02 1980-08-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-08-03 1984-02-02 1984-08-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-08-03 1988-02-02 1988-08-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag