Method of decolorizing sugar solutions with hybrid ion exchange resins
Assignee: Rohm and Haas Co
•
Filing: 1973-12-21
•
Granted: 1976-06-29
•
Expires: 1993-12-21
Abstract
Abstract Hybrid copolymers are prepared by at least partially filling the voids of a macroreticular copolymer with a gel-type, cross-linked copolymer of either the same monomers or a copolymer of different type monomers. The hybrid copolymers can be readily converted into ion exchange resins. Such resins have markedly improved physical and chemical properties, including improved ion exchange properties. Such resins are also especially useful for decolorizing sugar solutions.
Inventors
- 👤 James Henry Barrett
- 👤 David Henry Clemens
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 15:49
CPC Classifications
C; C13; C13B; C13B20/00; C13B20/14; B; B01; B01J; B01J47/00; B01J47/018; C08; C08F; C08F291/00; C08F8/00
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
105 words
A method of decolorizing sugar solutions which comprises contacting the solution with a hybrid ion exchange resin in which the resin has anionic exchange activity, said hybrid ion exchange resin being based on a hybrid copolymer comprising a cross-linked macroreticular porous host or base copolymer of a polyunsaturated monomer and a monoethylenically unsaturated monomer, said macroreticular copolymer being at least partially filled with a cross-linked gel copolymer of a polyunsaturated monomer and a monoethylenically unsaturated monomer, the gel copolymer or phase being present in the amount of about 5 to 300 parts by weight per 100 parts by weight of macroreticular host polymer or phase.
Claim 2
Independent Claim
105 words
A method of decolorizing sugar solutions which comprises contacting the solution with a hybrid ion exchange resin in which the resin has anionic exchange activity, said hybrid ion exchange resin being based on a hybrid copolymer comprising a cross-linked macroreticular porous host or base copolymer of a polyunsaturated monomer and a monoethylenically unsaturated monomer, said macroreticular copolymer being at least partially filled with a cross-linked gel copolymer of a polyunsaturated monomer and a monoethylenically unsaturated monomer, the gel copolymer or phase being present in the amount of about 5 to 300 parts by weight per 100 parts by weight of macroreticular host polymer or phase.
Claim 3
Dependent Claim
17 words
Method according to claim 1 wherein the resin ion exchange activity is quaternary ammonium ion exchange activity.
Claim 4
Dependent Claim
39 words
Method according to claim 2 wherein the resin is a quaternary ammonium anion exchange hybrid resin and wherein the host phase is a 3% divinylbenzene cross-linked-styrene macroreticular copolymer and the gel phase is a 1/2% divinylbenzene cross-linked-styrene gel copolymer.
Claim 5
Dependent Claim
31 words
Method according to claim 3 wherein the weight ratio of gel phase to the macroreticular phase is about 30 to 60 parts of gel phase per 100 parts of macroreticular phase.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1979-06-29 | 1979-12-29 | 1980-06-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1983-06-29 | 1983-12-29 | 1984-06-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1987-06-29 | 1987-12-29 | 1988-06-29 | $7700.00 | Window Closed / Lapsed |