Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
233 words
A process which comprises: a. reacting an aluminum-containing ore with hydrofluoric acid, fluosilicic acid or a mixture of hydrofluoric and fluosilicic acid, at a 0 to about 10% stoichiometric excess of acid and at a temperature of about 122° to about 212°F, to form a slurry containing aluminum fluoride in its liquid phase; b. separating the liquid phase containing the aluminum fluoride from the solid phase of the slurry; c. subjecting the separated liquid phase to crystallization to produce crystals of hydrated aluminum fluoride; d. separating the crystals from the crystallization mother liquor; e. drying and dehydrating the separate crystals, at a temperature of about 200°F to about 1400°F, to produce aluminum fluoride; f. pyrohydrolyzing the aluminum fluoride, at a temperature of about 1500°F to about 2500°F, to produce alumina and hydrofluoric acid; g. absorbing the hydrofluoric acid produced in step (f) in a first portion of the separated crystallization mother liquor, and recycling the fluorine enriched mother liquor to step (a) of the process; h. washing the separated crystals produced in step (d) and the separated solid phase of the slurry produced in step (b) with water, and recycling the water to step (a) of the process; and i. washing the separated solid phase of the slurry produced in step (b) with a second portion of the separated crystallization mother liquor, and recycling the mother liquor to step (a) of the process.
Claim 2
Dependent Claim
233 words
A process which comprises: a. reacting an aluminum-containing ore with hydrofluoric acid, fluosilicic acid or a mixture of hydrofluoric and fluosilicic acid, at a 0 to about 10% stoichiometric excess of acid and at a temperature of about 122° to about 212°F, to form a slurry containing aluminum fluoride in its liquid phase; b. separating the liquid phase containing the aluminum fluoride from the solid phase of the slurry; c. subjecting the separated liquid phase to crystallization to produce crystals of hydrated aluminum fluoride; d. separating the crystals from the crystallization mother liquor; e. drying and dehydrating the separate crystals, at a temperature of about 200°F to about 1400°F, to produce aluminum fluoride; f. pyrohydrolyzing the aluminum fluoride, at a temperature of about 1500°F to about 2500°F, to produce alumina and hydrofluoric acid; g. absorbing the hydrofluoric acid produced in step (f) in a first portion of the separated crystallization mother liquor, and recycling the fluorine enriched mother liquor to step (a) of the process; h. washing the separated crystals produced in step (d) and the separated solid phase of the slurry produced in step (b) with water, and recycling the water to step (a) of the process; and i. washing the separated solid phase of the slurry produced in step (b) with a second portion of the separated crystallization mother liquor, and recycling the mother liquor to step (a) of the process.
Claim 3
Dependent Claim
16 words
The process of claim 1 wherein step (a) is carried out at about 180° to 210°F.
Claim 4
Dependent Claim
16 words
The process of claim 1 wherein step (e) is carried out at about 800° to 1200°F.
Claim 5
Dependent Claim
16 words
The process of claim 1 wherein step (f) is carried out at about 1800° to 2500°F.
Claim 6
Dependent Claim
16 words
The process of claim 1 wherein step (c) is carried out at about 140° to 212°F.
Claim 7
Dependent Claim
232 words
A process which comprises: a. reacting an aluminum-containing clay with hydrofluoric acid, fluosilicic acid or a mixture of hydrofluoric and fluosilicic acid, at a 0 to about 10% stoichiometric excess of acid and at a temperature of about 122°F to about 212°F, to form a slurry containing aluminum fluoride in its liquid phase; b. separating the liquid phase containg the aluminum fluoride from the solid phase of the slurry; c. subjecting the separated liquid phase to crystallization to produce crystals of hydrated aluminum fluoride; d. separating the crystals from the crystallization mother liquor; e. drying and dehydrating the separated crystals, at a temperature of about 200°F to about 1400°F, to produce aluminum fluoride; f. pyrohydrolyzing the aluminum fluoride, at a temperature of about 1500°F to about 2500°F, to produce alumina and hydrofluoric acid; g. absorbing the hydrofluoric acid produced in step (f) in a first portion of the separated crystallization mother liquor, and recycling the fluorine-enriched mother liquor to step (a) of the process; h. washing the separated crystals produced in step (d) and the separated solid phase of the slurry produced in step (b) with water, and recycling the water to step (a) of the process; and i. washing the separated solid phase of the slurry produced in step (b) with a second portion of the separated crystallization mother liquor, and recycling the mother liquor to step (a) of the process.
Claim 8
Dependent Claim
232 words
A process which comprises: a. reacting an aluminum-containing clay with hydrofluoric acid, fluosilicic acid or a mixture of hydrofluoric and fluosilicic acid, at a 0 to about 10% stoichiometric excess of acid and at a temperature of about 122°F to about 212°F, to form a slurry containing aluminum fluoride in its liquid phase; b. separating the liquid phase containg the aluminum fluoride from the solid phase of the slurry; c. subjecting the separated liquid phase to crystallization to produce crystals of hydrated aluminum fluoride; d. separating the crystals from the crystallization mother liquor; e. drying and dehydrating the separated crystals, at a temperature of about 200°F to about 1400°F, to produce aluminum fluoride; f. pyrohydrolyzing the aluminum fluoride, at a temperature of about 1500°F to about 2500°F, to produce alumina and hydrofluoric acid; g. absorbing the hydrofluoric acid produced in step (f) in a first portion of the separated crystallization mother liquor, and recycling the fluorine-enriched mother liquor to step (a) of the process; h. washing the separated crystals produced in step (d) and the separated solid phase of the slurry produced in step (b) with water, and recycling the water to step (a) of the process; and i. washing the separated solid phase of the slurry produced in step (b) with a second portion of the separated crystallization mother liquor, and recycling the mother liquor to step (a) of the process.
Claim 9
Dependent Claim
15 words
The process of claim 6 wherein the aluminum-containing clay is a kaolin or montmorillonite clay.
Claim 10
Dependent Claim
245 words
A process which comprises: a. reacting uncalcined kaolin or montmorillonite clay with hydrofluoric acid, fluosilicic acid or a mixture of hydrofluoric and fluosilicic acid, at a 0 to about 10% stoichiometric excess acid and at a temperature of about 122°F to about 212°F, to form a slurry containing aluminum fluoride in its liquid phase; b. separating the liquid phase containing the aluminum fluoride from the solid phase of the slurry; c. subjecting the separated liquid phase to crystallization to produce crystals of hydrated aluminum fluoride; d. recycling a portion of the crystals to step (c) of the process; e. separating the remaining crystals from the crystallization mother liquor; f. drying and dehydrating the separated crystals, at a temperature of about 200°F to about 1400°F, to produce aluminum fluoride; g. pyrohydrolyzing the aluminum fluoride, at a temperature of about 1500°F to about 2500°F, to produce alumina and hydrofluoric acid; h. absorbing the hydrofluoric acid produced in step (g) in a first portion of the separated crystallization mother liquor, and recycling the fluorine-enriched mother liquor to step (a) of the process; i. washing the separated crystals produced in step (e) with water; j. combining the wash stream produced in step (i) with a second portion of the separated crystallization mother liquor to form a composite wash stream, washing the separated solid phase of the slurry produced in step (b) with the composite wash stream, and then recycling the composite wash stream to step (a) of the process.
Claim 11
Dependent Claim
245 words
A process which comprises: a. reacting uncalcined kaolin or montmorillonite clay with hydrofluoric acid, fluosilicic acid or a mixture of hydrofluoric and fluosilicic acid, at a 0 to about 10% stoichiometric excess acid and at a temperature of about 122°F to about 212°F, to form a slurry containing aluminum fluoride in its liquid phase; b. separating the liquid phase containing the aluminum fluoride from the solid phase of the slurry; c. subjecting the separated liquid phase to crystallization to produce crystals of hydrated aluminum fluoride; d. recycling a portion of the crystals to step (c) of the process; e. separating the remaining crystals from the crystallization mother liquor; f. drying and dehydrating the separated crystals, at a temperature of about 200°F to about 1400°F, to produce aluminum fluoride; g. pyrohydrolyzing the aluminum fluoride, at a temperature of about 1500°F to about 2500°F, to produce alumina and hydrofluoric acid; h. absorbing the hydrofluoric acid produced in step (g) in a first portion of the separated crystallization mother liquor, and recycling the fluorine-enriched mother liquor to step (a) of the process; i. washing the separated crystals produced in step (e) with water; j. combining the wash stream produced in step (i) with a second portion of the separated crystallization mother liquor to form a composite wash stream, washing the separated solid phase of the slurry produced in step (b) with the composite wash stream, and then recycling the composite wash stream to step (a) of the process.