Abstract In a staged calcination process a sulfur-containing green coke is converted to a low-sulfur-content coke and two off-gas streams, one which contains sulfur dioxide and another which contains hydrogen sulfide. In one stage the green coke is calcined and partially desulfurized under oxidative conditions at a temperature in the range 1000 DEG to 3000 DEG F. In a second stage, the calcination and desulfurization is continued by heating the coke from 2000 DEG to 4000 DEG F under substantially reducing conditions. Preferably the reaction times and conditions in the stages are adjusted to result in the production of two mols of hydrogen sulfide per mol of sulfur dioxide. Portions of the two off-gas streams are mixed and reacted to form elemental sulfur.
A process for the production of a calcined low-sulfur-content coke and elemental sulfur from a green coke having a substantial sulfur content which comprises: a. producing a sulfur dioxide-containing off-gas and a partially desulfurized coke by calcining said green coke under oxidative conditions including a temperature in the range 1000°to 3000°F, b. producing a hydrogen sulfide-containing off-gas and said low-sulfur-content coke by calcining said partially desulfurized coke under reducing conditions including a temperature in the range 2000°to 4000°F; and c. forming elemental sulfur and water by combining and reacting at least a portion of said sulfur dioxide-containing off-gas with at least a portion of said hydrogen sulfide-containing off-gas.
Claim 2
Dependent Claim
108 words
A process for the production of a calcined low-sulfur-content coke and elemental sulfur from a green coke having a substantial sulfur content which comprises: a. producing a sulfur dioxide-containing off-gas and a partially desulfurized coke by calcining said green coke under oxidative conditions including a temperature in the range 1000°to 3000°F, b. producing a hydrogen sulfide-containing off-gas and said low-sulfur-content coke by calcining said partially desulfurized coke under reducing conditions including a temperature in the range 2000°to 4000°F; and c. forming elemental sulfur and water by combining and reacting at least a portion of said sulfur dioxide-containing off-gas with at least a portion of said hydrogen sulfide-containing off-gas.
Claim 3
Dependent Claim
43 words
The process of claim 1 wherein the rates of production of said sulfur dioxide-containing off-gas and said hydrogen sulfide-containing off-gas are controlled to produce hydrogen sulfide and sulfur dioxide in approximately the stoichiometric amounts necessary for the reaction to form said elemental sulfur.
Claim 4
Dependent Claim
18 words
The process of claim 1 wherein said oxidative conditions include a temperature in the range 2000° to 2500°F.
Claim 5
Dependent Claim
18 words
The process of claim 1 wherein said reducing conditions include a temperature in the range 2500° to 3000°F.
Claim 6
Dependent Claim
31 words
A process of claim 2 wherein said oxidative conditions include a temperature in the range 2000° to 2500°F and said reducing conditions include a temperature in the range 2500° to 3000°F.
Claim 7
Dependent Claim
30 words
The process of claim 5 wherein said hydrogen sulfide off-gas is formed by heating said partially desulfurized coke in an electrothermal resistance furnace in the substantial absence of oxygen-containing compounds.