Abstract

Abstract A process in which copper, nickel, cobalt and molybdenum are recovered by leaching comminuted raw manganese nodules with an aqueous ammoniacal leach solution containing cuprous ions. An improvement is disclosed in which the metal values are extracted directly from the leach slurry with an organic extractant. To accomplish such extraction the amount by weight of solids in the slurry is maintained at less than 20 percent, the pH of the slurry is lowered to 9.5, the volumes of slurry and organic are maintained at a ratio so that the organic is the continuous phase and the organic and slurry are mixed with gentle agitation.

Inventors

  • 👤 J. Paul Pemsler
  • 👤 John K. Litchfield

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 07:06
CPC Classifications
C; C22; C22B; C22B47/00; C22B47/0018; C22B47/0045; C22B47/0081; C01; C01G; C01G3/00; C01G3/003; C01G53/00; C01G53/01; C22B15/00; C22B15/0063; C22B15/0065; C22B15/0078; C22B3/00; C22B3/04; C22B3/12; C22B3/14; C22B3/20; C22B3/26; C22B3/30; C22B34/00; C22B34/30; C22B34/34; C22B47/0054; C22B47/0072; Y; Y02; Y02P; Y02P10/00; Y02P10/20; Y10; Y10S; Y10S423/00; Y10S423/04

Claims Analysis

Total Claims: 18
Claim 1
Independent Claim 201 words
A process for the recovery of base metal values selected from the group consisting of copper and nickel from a manganese containing ore comprising introducing a stream of said manganese containing ore into a reaction vessel containing cuprous ions in an aqueous ammoniacal ammonium carbonate solution to enable the cuprous ions to reduce the manganese oxides in the ore and solubilize the metal values therein, delivering reduced manganese ore slurry from the reaction vessel to a mixer/settler, lowering the pH of the slurry to at least 10.0, but not lower than 8.5, maintaining the amount of solid in the slurry in the mixer at 20% by weight or less, introducing an organic extractant capable of extracting copper and nickel values from aqueous ammonical ammonium carbonate solutions at pH's between 8.5-10 into the mixer/settler, the volume of slurry and organic extractant being maintained at a ratio so that the organic extractant in the mixer is in the continuous phase and extracting the base metal values from the slurry with the extractant, the control of pH, solid content of the slurry and mixer operation enabling metal values to be extracted from slurries with losses of organic reagents held to 100-200 parts per million.
Claim 2
Dependent Claim 201 words
A process for the recovery of base metal values selected from the group consisting of copper and nickel from a manganese containing ore comprising introducing a stream of said manganese containing ore into a reaction vessel containing cuprous ions in an aqueous ammoniacal ammonium carbonate solution to enable the cuprous ions to reduce the manganese oxides in the ore and solubilize the metal values therein, delivering reduced manganese ore slurry from the reaction vessel to a mixer/settler, lowering the pH of the slurry to at least 10.0, but not lower than 8.5, maintaining the amount of solid in the slurry in the mixer at 20% by weight or less, introducing an organic extractant capable of extracting copper and nickel values from aqueous ammonical ammonium carbonate solutions at pH's between 8.5-10 into the mixer/settler, the volume of slurry and organic extractant being maintained at a ratio so that the organic extractant in the mixer is in the continuous phase and extracting the base metal values from the slurry with the extractant, the control of pH, solid content of the slurry and mixer operation enabling metal values to be extracted from slurries with losses of organic reagents held to 100-200 parts per million.
Claim 3
Dependent Claim 26 words
The process as set forth in claim 1 wherein an oxime extractant is introduced into the mixer/settler to extract the base metal values from the slurry.
Claim 4
Dependent Claim 29 words
The process as set forth in claim 1 wherein the slurry and extractant are mixed in the mixer at speeds sufficiently slow so the formation of emulsions are avoided.
Claim 5
Dependent Claim 26 words
The process as set forth in claim 3 wherein an oxime extractant is introduced into the mixer/settler to extract the base metal values from the slurry.
Claim 6
Dependent Claim 32 words
The process as set forth in claim 3 including the step of oxidizing the slurry to convert the cuprous ions to cupric ions said oxidation being performed prior to the extracting step.
Claim 7
Dependent Claim 26 words
The process as set forth in claim 5 wherein an oxime extractant is introduced into the mixer/settler to extract the base metal values from the slurry.
Claim 8
Dependent Claim 29 words
The process as set forth in claim 3 wherein the slurry is maintained at 20% by weight or less by diluting the slurry with ammonia, carbon dioxide and water.
Claim 9
Dependent Claim 26 words
The process as set forth in claim 7 wherein an oxime extractant is introduced into the mixer/settler to extract the base metal values from the slurry.
Claim 10
Dependent Claim 25 words
The process as set forth in claim 3 wherein the extractant to slurry volume ratio is maintained at 2 to 1 during the mixing step.
Claim 11
Dependent Claim 26 words
The process as set forth in claim 9 wherein an oxime extractant is introduced into the mixer/settler to extract the base metal values from the slurry.
Claim 12
Dependent Claim 18 words
The process as set forth in claim 3 wherein the pH of the slurry is lowered to 9.3.
Claim 13
Dependent Claim 26 words
The process as set forth in claim 11 wherein an oxime extractant is introduced into the mixer/settler to extract the base metal values from the slurry.
Claim 14
Dependent Claim 197 words
A process for extracting at least one metal value selected from the group consisting of copper and nickel directly from a slurry which contains solids and an ammoniacal solution containing the metal values to be extracted comprising the following steps: a. adjusting the pH of the slurry to a value of 10.0 or lower, but not lower than 8.5; b. diluting the slurry so that the solid content of the slurry is at a value of 20% by weight or less; c. contacting the slurry with an organic extractant capable of extracting said copper and nickel metal values from said ammoniacal leach solutions having pH's between 8.5 and 10, the volume of organic extractant being selected so that the system is in an organic-continuous phase; d. agitating the slurry to increase contact between the organic extractant and the slurry without causing the formation of emulsions; and, e. separating the extractant from the slurry to yield an organic extractant loaded with said copper and nickel metal values; the control of pH, solid content of the slurry and mixer operation enabling metal values to be extracted from slurries with losses of organic reagents held to 100-200 parts per million.
Claim 15
Dependent Claim 197 words
A process for extracting at least one metal value selected from the group consisting of copper and nickel directly from a slurry which contains solids and an ammoniacal solution containing the metal values to be extracted comprising the following steps: a. adjusting the pH of the slurry to a value of 10.0 or lower, but not lower than 8.5; b. diluting the slurry so that the solid content of the slurry is at a value of 20% by weight or less; c. contacting the slurry with an organic extractant capable of extracting said copper and nickel metal values from said ammoniacal leach solutions having pH's between 8.5 and 10, the volume of organic extractant being selected so that the system is in an organic-continuous phase; d. agitating the slurry to increase contact between the organic extractant and the slurry without causing the formation of emulsions; and, e. separating the extractant from the slurry to yield an organic extractant loaded with said copper and nickel metal values; the control of pH, solid content of the slurry and mixer operation enabling metal values to be extracted from slurries with losses of organic reagents held to 100-200 parts per million.
Claim 16
Dependent Claim 21 words
The process as set forth in claim 13 wherein in step (c), the slurry is contacted with an organic oxime extractant.
Claim 17
Dependent Claim 24 words
The process as set forth in claim 13 wherein in step (c) the extractant to slurry volume ratio is maintained at 2 to 1.
Claim 18
Dependent Claim 21 words
The process as set forth in claim 15 wherein in step (c), the slurry is contacted with an organic oxime extractant.

References Cited (Backward Citations)

US3206288A Cited
US3224873A Cited
US3761249A Cited
US3743585A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-04-13 1979-10-13 1980-04-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-04-13 1983-10-13 1984-04-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-04-13 1987-10-13 1988-04-13 $7700.00 Window Closed / Lapsed