Abstract

Abstract Disclosed is a method particularly useful in fabricating microwave components for joining two metallic surfaces together to form an extremely strong bond, having good electrical and mechanical characteristics. One surface is primed or prepared with a suitable primer. An alloy adhesive, such as a polyamide-epoxy, is either deposited on the prepared surface or, if the adhesive is in film form on a release paper, then the film and release paper are heat tacked or ironed onto the prepared metallic surface. The paper release backing is then removed and the two metallic surfaces are mechanically assembled and positioned within a vacuum bag. The bag is evacuated and subjected to normal atmospheric pressure (14 psi) and heated to approximately 350° for 1 hour whereupon the component is allowed to cool to 100°F at which time the vacuum may be released and the component removed from the bag.

Inventors

  • 👤 Warren D. Williams

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 21:43
CPC Classifications
B; B29; B29C; B29C66/00; B29C66/80; B29C66/81; B29C66/814; B29C66/8145; B29C66/81455; B29C65/00; B29C65/02; B29C65/18; B29C65/48; B29C65/4805; B29C65/483; B29C65/4835; H; H01; H01P; H01P11/00; H01Q; H01Q21/00; H01Q21/0006; H01Q21/0037; H01Q21/0043; H01Q21/005; B29C66/50; B29C66/51; B29C66/54

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 169 words
A method of bonding together sections of aluminum surfaces for fabricating a slotted waveguide type antenna which comprises: a. priming one of the aluminum surfaces of one of two antenna sections to be joined, and applying an adhesive film less than 1 mil thick to the primed aluminum surface of the two antenna sections, wherein the primed aluminum surface of one of the sections to be joined is a slotted flat plate and the second section is a plurality of thin wall waveguide shunt guides; b. contacting the aluminum surfaces to combine the primer and adhesive material between the aluminum surfaces of the two antenna sections to be bonded together; c. positioning the contacting sections in a vacuum bag adaptable, when subject to a vacuum, to the form of the antenna sections; d. evacuating the vacuum bag to exert a selected uniform bonding pressure on the antenna section; and e. heating said vacuum bag containing the antenna sections to an adhesive curing temperature to bond together the antenna sections.
Claim 2
Independent Claim 169 words
A method of bonding together sections of aluminum surfaces for fabricating a slotted waveguide type antenna which comprises: a. priming one of the aluminum surfaces of one of two antenna sections to be joined, and applying an adhesive film less than 1 mil thick to the primed aluminum surface of the two antenna sections, wherein the primed aluminum surface of one of the sections to be joined is a slotted flat plate and the second section is a plurality of thin wall waveguide shunt guides; b. contacting the aluminum surfaces to combine the primer and adhesive material between the aluminum surfaces of the two antenna sections to be bonded together; c. positioning the contacting sections in a vacuum bag adaptable, when subject to a vacuum, to the form of the antenna sections; d. evacuating the vacuum bag to exert a selected uniform bonding pressure on the antenna section; and e. heating said vacuum bag containing the antenna sections to an adhesive curing temperature to bond together the antenna sections.
Claim 3
Independent Claim 168 words
A method of bonding together metal surfaces of microwave waveguide sections for fabricating light weight microwave waveguides or the like which comprises: a. priming the metal surfaces of the sections; b. applying an adhesive film less than one mil thick on a backing material to the primed metal surface to a first one of the sections to be bonded together to insure proper positioning and uniform thickness of the bonding material for alleviating bridging and warping of the bonded sections; c. removing the backing material from the adhesive film; d. contacting the primed metal surface of a second section to be bonded to the adhesive film carried by the first section; e. positioning the contacting sections in a vacuum bag adaptable, when subjected to a vacuum, to the form of the contacting sections; f. evacuating said vacuum bag to exert a uniform pressure of about 14 psi on the sections; and g. heating said vacuum bag containing the sections to a curing temperature to bond the sections together.
Claim 4
Independent Claim 168 words
A method of bonding together metal surfaces of microwave waveguide sections for fabricating light weight microwave waveguides or the like which comprises: a. priming the metal surfaces of the sections; b. applying an adhesive film less than one mil thick on a backing material to the primed metal surface to a first one of the sections to be bonded together to insure proper positioning and uniform thickness of the bonding material for alleviating bridging and warping of the bonded sections; c. removing the backing material from the adhesive film; d. contacting the primed metal surface of a second section to be bonded to the adhesive film carried by the first section; e. positioning the contacting sections in a vacuum bag adaptable, when subjected to a vacuum, to the form of the contacting sections; f. evacuating said vacuum bag to exert a uniform pressure of about 14 psi on the sections; and g. heating said vacuum bag containing the sections to a curing temperature to bond the sections together.
Claim 5
Dependent Claim 41 words
A method of bonding together metal surfaces of microwave waveguide sections according to claim 2, wherein said vacuum bag containing the sections to be joined is heated to a temperature of about 350°F for about 1 hour to form a waveguide.
Claim 6
Dependent Claim 36 words
A method of bonding together metal surfaces of microwave waveguide sections according to claim 3, wherein the temperature is allowed to fall after about 1 hour to about 100°F prior to removal of the waveguide sections.

References Cited (Backward Citations)

US3481814A Cited
US3706621A Cited
US3723223A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-04-13 1979-10-13 1980-04-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-04-13 1983-10-13 1984-04-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-04-13 1987-10-13 1988-04-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag