← Back to Patent Explorer
US3941182A Expired / Lapsed US ⏱️ 0.0 years remaining

Continuous process for preparing unidirectionally reinforced metal foam

Assignee: Individual
•
Filing: 1973-07-31
•
Granted: 1976-03-02
•
Expires: 1993-07-31
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Steel wires are pulled through a reactor tube in which they continuously interact with a foaming metal mass. The steel wires are coated with a metal which forms a binary alloy with the matrix metal, thereby protecting the steel from being dissolved. The foaming matrix metal is usually an aluminum alloy but can be any light or low melting metal including zinc or lead. The steel wires protect the metal foam from cracking in the pultrusion process.

Inventors

  • 👤 Johan Bjorksten
  • 👤 Edward J. Rock

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 20:32
CPC Classifications
B; B22; B22D; B22D11/00; B22D25/00; B22D25/005; C; C22; C22C; C22C1/00; C22C1/08; C22C47/00; C22C47/02; C22C47/06; C22C47/062; C22C47/066; C22C47/08; C22C1/083; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12479; Y10T428/12493; Y10T428/12736; Y10T428/1275

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 222 words
The process of providing a longitudinally elongated body of metal foam having longitudinally extending wires therewithin, said wires being of metal melting higher than the metal of the foam, comprising the combination of the steps of: 1. intensively mixing into molten metal to be foamed a substance which decomposes and liberates gas when heated, and 2. heating said substance to decompose it while it is immersed in said molten metal to produce molten metal foam with heat by conduction from said molten metal, 3. moving said molten metal foam longitudinally to provide a longitudinally moving body of molten metal foam, 4. providing said longitudinally moving body of molten metal foam between a plurality of longitudinally moving surfaces of endless metal belts contacting said longitudinally moving body of molten metal foam, 5. providing a plurality of metal wires of metal melting higher than the metal of said foam, said wires having surfaces disposed to adhere to the metal of said foam, 6. moving said wires longitudinally to introduce said wires longitudinally into said longitudinally moving body of molten metal foam with said wires moving longitudinally at the same longitudinal rate as the rate of longitudinal movement of said longitudinally moving body of molten metal foam, 7. cooling said longitudinally moving body of metal foam containing said wires to provide said longitudinally elongated body.
Claim 2
Dependent Claim 222 words
The process of providing a longitudinally elongated body of metal foam having longitudinally extending wires therewithin, said wires being of metal melting higher than the metal of the foam, comprising the combination of the steps of: 1. intensively mixing into molten metal to be foamed a substance which decomposes and liberates gas when heated, and 2. heating said substance to decompose it while it is immersed in said molten metal to produce molten metal foam with heat by conduction from said molten metal, 3. moving said molten metal foam longitudinally to provide a longitudinally moving body of molten metal foam, 4. providing said longitudinally moving body of molten metal foam between a plurality of longitudinally moving surfaces of endless metal belts contacting said longitudinally moving body of molten metal foam, 5. providing a plurality of metal wires of metal melting higher than the metal of said foam, said wires having surfaces disposed to adhere to the metal of said foam, 6. moving said wires longitudinally to introduce said wires longitudinally into said longitudinally moving body of molten metal foam with said wires moving longitudinally at the same longitudinal rate as the rate of longitudinal movement of said longitudinally moving body of molten metal foam, 7. cooling said longitudinally moving body of metal foam containing said wires to provide said longitudinally elongated body.
Claim 3
Dependent Claim 31 words
The process of claim 1 characterized by providing said wires of steel and coating said wires with brass before introducing the wires into said longitudinally moving body of molten metal foam.

References Cited (Backward Citations)

US275408A Cited
US3126595A Cited
US867659A Cited
FR615147A Cited
US2849790A Cited
US2937938A Cited
GB901917A Cited
US3005700A Cited
US3306716A Cited
US3733382A Cited
US3756303A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-03-02 1979-09-01 1980-03-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-03-02 1983-09-01 1984-03-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-03-02 1987-09-01 1988-03-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag