Abstract

Abstract A low-pressure mercury vapour discharge lamp provided with a luminescent coating comprising three luminescent materials each emitting in a narrow spectral range. The first material has an emission band with a maximum between 430 and 490 nm; the second material has its emission in the range 520-565 nm; the third material emits in the range 590-630 nm. The second material is defined by one of the formulas: A. Ce 1-x-y La x Tb y MgAl 11 O 19 b. (Ce 1-x-y La x Tb y ) 2 O 3 .nAl 2 O 3 The first material is preferably chosen from C. A 1-p Eu p Mg 2-q Mn q Al 16 O 27 d. B 5 .5-x Eu x Mg 6-y Mn y Al 55 O 94 (a and B are barium and/or strontium).

Inventors

  • 👤 Judicus Marinus Pieter Jan Verstegen
  • 👤 Dragutin Radielovic
  • 👤 Lambertus Wilhelmus Johannes Manders

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 02:06
CPC Classifications
H; H01; H01J; H01J61/00; H01J61/02; H01J61/38; H01J61/42; H01J61/44; C; C09; C09K; C09K11/00; C09K11/08; C09K11/70; C09K11/71; C09K11/74; C09K11/75; C09K11/76; C09K11/77; C09K11/7766; C09K11/7774; C09K11/7783; C09K11/7784; C09K11/7787

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 216 words
A low-pressure mercury vapour discharge lamp having a vacuum tight radiation transmitting envelope comprising a quantity of mercury and a quantity of rare gas and provided with electrodes between which the discharge takes place during operation, and with a luminescent coating comprising three luminescent materials, a first material having an emission band at a maximum in the wavelength range between 430 and 490 nm and a half value width of less than 100 nm, a second material mainly having its emission in the wavelength range between 520 nm and 565 nm, and a third material mainly having its emission in the wavelength range between 590 and 630 nm, wherein said second luminescent material is activated by terbium and is selected from the group consisting of materials defined by the formulas: Ce.sub.1-x-y La.sub.x Tb.sub.y MgAl.sub.11 O.sub.19 and a (Ce.sub.1-x-y La.sub.x Tb.sub. y).sub.2 O.sub.3.sup.. nAl.sub.2 O.sub.3 b in which O ≦ x ≦ 0.50 0.20 ≦ y ≦ 0.50 x+y ≦ 0.90 10 ≦ n ≦ 12 and in which up to a maximum of 25 at% of aluminum may be replaced by elements selected from the group consisting of gallium and scandium and in which magnesium may at least in part be replaced by one or more elements selected from the group consisting of zinc and beryllium.
Claim 2
Dependent Claim 216 words
A low-pressure mercury vapour discharge lamp having a vacuum tight radiation transmitting envelope comprising a quantity of mercury and a quantity of rare gas and provided with electrodes between which the discharge takes place during operation, and with a luminescent coating comprising three luminescent materials, a first material having an emission band at a maximum in the wavelength range between 430 and 490 nm and a half value width of less than 100 nm, a second material mainly having its emission in the wavelength range between 520 nm and 565 nm, and a third material mainly having its emission in the wavelength range between 590 and 630 nm, wherein said second luminescent material is activated by terbium and is selected from the group consisting of materials defined by the formulas: Ce.sub.1-x-y La.sub.x Tb.sub.y MgAl.sub.11 O.sub.19 and a (Ce.sub.1-x-y La.sub.x Tb.sub. y).sub.2 O.sub.3.sup.. nAl.sub.2 O.sub.3 b in which O ≦ x ≦ 0.50 0.20 ≦ y ≦ 0.50 x+y ≦ 0.90 10 ≦ n ≦ 12 and in which up to a maximum of 25 at% of aluminum may be replaced by elements selected from the group consisting of gallium and scandium and in which magnesium may at least in part be replaced by one or more elements selected from the group consisting of zinc and beryllium.
Claim 3
Dependent Claim 33 words
A low-pressure mercury vapour discharge lamp as claimed in claim 1, wherein said second luminescent material is defined by formula (a) and 0 ≦ x ≦ 0.20 and 0.20 ≦ y ≦ 0.40.
Claim 4
Dependent Claim 21 words
A low-pressure mercury vapour discharge lamp as claimed in claim 1, wherein said first luminescent material is activated by bivalent europium.
Claim 5
Dependent Claim 66 words
A low-pressure mercury vapour discharge lamp as claimed in claim 3, wherein said first luminescent material is an aluminate of an element selected from the group consisting of barium and strontium activated by a material selected from the group consisting of (1) bivalent europium and (2) bivalent europium and bivalent manganese, which aluminate has a hexagonal crystal structure akin to the structure of the hexagonal ferrites.
Claim 6
Dependent Claim 121 words
A low-pressure mercury vapour discharge lamp as claimed in claim 4, wherein said first luminescent material is a ternary aluminate of an element of the group consisting of barium, strontium and magnesium in which the atomic fraction of aluminum is larger than 1.8 times the atomic fraction of magnesium and is also larger than 3.7 times the atomic fraction of the element selected from the group consisting of barium and strontium and in which up to a maximum of 25 at% of aluminum may be replaced by an element selected from the group consisting of gallium and scandium and in which magnesium may at least in part be replaced by an element selected from the group consisting of zinc and beryllium.
Claim 7
Dependent Claim 89 words
A low-pressure mercury vapour discharge lamp as claimed in claim 5 characterized in that said first luminescent material is selected from the group consisting of materials defined by the formulas: A.sub.1-p Eu.sub.p Mg.sub.2-q Mn.sub.q Al.sub.16 O.sub.27 and C B.sub.5.5-x Eu.sub.x Mg.sub.6-y Mn.sub.y Al.sub.55 O.sub.94 D in which A and B represent at least one of the elements selected from the group consisting of barium and strontium and in which 0.05 ≦ p ≦ 0.20 0.25 ≦ x ≦ 1.50 0 ≦ g/p ≦ 1.5 0 ≦ y/x ≦ 1.5
Claim 8
Dependent Claim 29 words
A low-pressure mercury vapour discharge lamp as claimed in claim 6, wherein at least 50 at% of A is barium and at least 50 at% of B is strontium.
Claim 9
Dependent Claim 52 words
A low-pressure mercury vapour discharge lamp as claimed in claim 1 in which said third luminescent material is a rare earth oxide activated by trivalent europium and defined by the formula Ln 2 O 3 :Eu 3 + in which Ln represents at least one of the elements yttrium, gadolinium and lutetium.
Claim 10
Dependent Claim 61 words
A low-pressure mercury vapour discharge lamp as claimed in claim 1 wherein said luminescent coating comprises at least one of the luminescent materials selected from the group consisting of antimony-activated alkaline earth halofosfate, antimony and manganese-activated alkaline earth halofosfate, tin-activated alkaline earth magnesium orthofosfate, manganese-activated magnesium arsenate and manganese-activated magnesium germanate in a quantity of not more than 50% by weight.

References Cited (Backward Citations)

US3114067A Cited
US3858082A Cited
US3748517A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-02-09 1979-08-11 1980-02-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-02-09 1983-08-11 1984-02-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-02-09 1987-08-11 1988-02-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag