Patent CH475876A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3933486A Expired / Lapsed US ⏱️ 0.0 years remaining

Silver-metal oxide composite and method of manufacturing the same

Assignee: Chugai Electric Industrial Co Ltd
•
Filing: 1974-05-30
•
Granted: 1976-01-20
•
Expires: 1994-05-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An electrical contact material obtained through internally oxidizing a silver alloy which is the solid solution with 5 to 20 weight percent of one or more of the solute metal elements selected from tin, zinc and antimony and which contains 0.01 to 1.0% weight percent of bismuth. The silver alloy may also include up to 0.5 weight percent of ferrous metal or metals.

Inventors

  • 👤 Akira Shibata

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 19:41
CPC Classifications
H; H01; H01H; H01H1/00; H01H1/02; H01H1/021; H01H1/023; H01H1/0237; H01H1/02372; C; C22; C22C; C22C5/00

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 63 words
An electrical contact material obtained by internally oxidizing an alloy of silver and solute metal elements, said alloy comprising a silver matrix, 5 to 20 weight percent of one or more of solute metal elements selected from the group consisting of tin, zinc, and antimony, and as an essential material, 0.01 to 1.0 weight percent of bismuth precipitated in the alloy as oxides.
Claim 2
Dependent Claim 63 words
An electrical contact material obtained by internally oxidizing an alloy of silver and solute metal elements, said alloy comprising a silver matrix, 5 to 20 weight percent of one or more of solute metal elements selected from the group consisting of tin, zinc, and antimony, and as an essential material, 0.01 to 1.0 weight percent of bismuth precipitated in the alloy as oxides.
Claim 3
Dependent Claim 47 words
The material as claimed in claim 1 wherein the maximum diameter of the grain boundaries of the silver matrix is less than 50 μ, and thin films of the oxides of tin, zinc or antimony and of the oxides of bismuth are precipitated in said grain boundaries.
Claim 4
Dependent Claim 17 words
The material as claimed in claim 1 further containing less than 0.5 weight percent of ferrous metals.

References Cited (Backward Citations)

US2200855A Cited
US2496555A Cited
US2486341A Cited
US2861155A Cited
DE1153178B Cited
US3323911A Cited
DE2011002A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-01-19 1979-07-21 1980-01-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-01-19 1983-07-21 1984-01-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-01-19 1987-07-21 1988-01-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag