Abstract

Abstract Photolithographic techniques are employed to fabricate hemispherical or semicylindrical microlenses on the end surfaces of optical fibers. The power coupling efficiency between junction lasers and fibers is thereby significantly increased.

Inventors

  • 👤 Leonard George Cohen
  • 👤 Martin Victor Schneider

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 15:58
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/24; G02B6/42; G02B6/4201; G02B6/4202; G02B6/4203; G03; G03F; G03F7/00; G03F7/0005

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 158 words
A method for forming a microlens on one end surface of an optical fiber that comprises a relatively high index-of-refraction cylindrical core having a relatively low index-of-refraction cladding disposed thereabout, said method comprising the steps of: coating the entire surface of said one end of said fiber with a negative transparent photoresist material, exposing to radiation only a selected portion of the material coated on said end surface by directing at said material a radiant beam whose cross-sectional area approximates that of said core and is much less than the cross-sectional area of said core and cladding, said selected portion including the material that covers the entire core area of the fiber but excludes the major portion of the material that covers the cladding of the fiber, removing the unexposed portion of said material, and baking said remaining exposed portion to cause it to flow slightly, thereby to harden said exposed portion and to smooth the contour thereof.
Claim 2
Independent Claim 158 words
A method for forming a microlens on one end surface of an optical fiber that comprises a relatively high index-of-refraction cylindrical core having a relatively low index-of-refraction cladding disposed thereabout, said method comprising the steps of: coating the entire surface of said one end of said fiber with a negative transparent photoresist material, exposing to radiation only a selected portion of the material coated on said end surface by directing at said material a radiant beam whose cross-sectional area approximates that of said core and is much less than the cross-sectional area of said core and cladding, said selected portion including the material that covers the entire core area of the fiber but excludes the major portion of the material that covers the cladding of the fiber, removing the unexposed portion of said material, and baking said remaining exposed portion to cause it to flow slightly, thereby to harden said exposed portion and to smooth the contour thereof.
Claim 3
Dependent Claim 46 words
A method as in claim 1 wherein said exposing step comprises directing radiation into the other end of said fiber to propagate along said core to impinge on the rear surface of said material only in the area overlying said core and the immediate vicinity thereof.
Claim 4
Dependent Claim 122 words
A method as in claim 1 wherein said exposing step comprises: during a first interval of time directing a rectangular beam of radiation to impinge on the front surface of said material in a centrally positioned location overlying said core, the cross-sectional area of said beam being much less than the cross-sectional area of said core and cladding, and during a second interval of time directing a wider rectangular beam of sensitizing light to impinge on the front surface of said material in a centrally positioned location overlying said core, the cross-sectional area of said wider beam being much less than the cross-sectional area of said core and cladding and substantially encompassing within it the cross-sectional area of said first-recited rectangular beam.
Claim 5
Dependent Claim 28 words
A method as in claim 3 wherein said exposing step includes focusing each of said beams in a plane that is spaced in front of said front surface.
Claim 6
Dependent Claim 50 words
A method as in claim 4 wherein said exposing step is preceded by the step of directing nonsensitizing light into the other end of the said fiber to illuminate the core at said one end to provide a reference spot for aligning said rectangular beams in said centrally positioned location.

References Cited (Backward Citations)

US3658528A Cited
US3771983A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-01-12 1979-07-14 1980-01-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-01-12 1983-07-14 1984-01-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-01-12 1987-07-14 1988-01-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag