Flame-resistant polyolefin used as insulator for electrical conductors

Assignee: Vulkor Inc
•
Filing: 1974-10-21
•
Granted: 1975-12-30
•
Expires: 1994-10-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An electrical conductor insulated with flame-resistant polyolefin compositions comprising the combination of phosphorylated Novolak-type phenol-formaldehyde condensate and triallyl cyanurate, and method of producing same.

Inventors

  • 👤 Jr Burton Thornley Mackenzie
  • 👤 Edward Vincent Wilkus

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 15:29
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/16; C08K5/34; C08K5/3467; C08K5/3477; C08G; C08G8/00; C08G8/28; C08K3/00; C08K3/02; C08K3/04; C08K3/34; C08K3/346; C08K5/3492; C08K5/34924; C08L; C08L23/00; C08L23/02; C08L23/04; C08L23/06; C08L61/00; C08L61/04; C08L61/06; C08L61/14; H; H01; H01B; H01B3/00; H01B3/18; H01B3/30; H01B3/44; H01B3/441; H01B7/00; H01B7/17; H01B7/29; H01B7/295; C08K5/04; C08K5/14; C08L2201/00; C08L2201/02; C08L2203/00; C08L2203/20; C08L2203/202; C08L2312/00; C08L2666/00; C08L2666/02; C08L2666/14; C08L2666/16; Y; Y10; Y10S; Y10S260/00; Y10S260/24; Y10T; Y10T428/00; Y10T428/29; Y10T428/2913; Y10T428/2933; Y10T428/294; Y10T428/31504; Y10T428/31678; Y10T428/31688; Y10T428/31692

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 26 words
AN INSULATED ELECTRICAL CONSUCTOR INCLUDING A METALLIC ELEMENT HAVING THEREABOUT AN INSULATION OF FLAME-RESISTANT POLYOLEFIN COMPOUND COMPRISING THE COMBINATION OF PHOSPHORYLATED NOVAK PHENOL-FORMALDEHYDE AND TRIALLYL CYANURATE.
Claim 2
Dependent Claim 26 words
AN INSULATED ELECTRICAL CONSUCTOR INCLUDING A METALLIC ELEMENT HAVING THEREABOUT AN INSULATION OF FLAME-RESISTANT POLYOLEFIN COMPOUND COMPRISING THE COMBINATION OF PHOSPHORYLATED NOVAK PHENOL-FORMALDEHYDE AND TRIALLYL CYANURATE.
Claim 3
Dependent Claim 47 words
THE INSULATED ELECTRICAL CONDUCTOR OF CLAIM 1, WHEREIN THE POLYOLEFIN COMPOUND OF THE INSULATION COMPRISES ABOUT 5 TO ANOUT 10 PARTS BY WEIGHT OF PHOSPHORYLATED NOVOK PHENOL-FORMALDEHYDE AND ABOUT 0.5 TO ABOUT 5 PARTS BY WEIGHT OF TRIALLYL CYANURATE PER 100 PARTS BY WEIGHT OF THE POLYOLEFIN.
Claim 4
Dependent Claim 36 words
The insulated electrical conductor of claim 1, wherein the polyolefin compound comprises at least one ethylene-containing polymer selected from the group consisting of polyethylene, copolymers of ethylene and other polymerizable materials, and blends of such polymers.
Claim 5
Dependent Claim 74 words
An insulated electrical conductor including a metallic element having thereabout an insulation of flame-resistant polyolefin compound comprising at least one ethylene-containing polymer selected from the group consisting of polyethylene, copolymers of ethylene and other polymerizable materials, and blends of such polymers, about 5 to about 20 parts by weight of phosphorylated novolak phenol-formaldehyde and about 0.5 to about 5 parts by weight of triallyl cyanurate per 100 parts by weight of the ethylene-containing polymer.
Claim 6
Dependent Claim 74 words
An insulated electrical conductor including a metallic element having thereabout an insulation of flame-resistant polyolefin compound comprising at least one ethylene-containing polymer selected from the group consisting of polyethylene, copolymers of ethylene and other polymerizable materials, and blends of such polymers, about 5 to about 20 parts by weight of phosphorylated novolak phenol-formaldehyde and about 0.5 to about 5 parts by weight of triallyl cyanurate per 100 parts by weight of the ethylene-containing polymer.
Claim 7
Dependent Claim 29 words
The insulated electrical conductor of claim 4, wherein the ethylene-containing polymer has been crosslink cured to a substantially thermoset condition with a free radical forming organic peroxide curing agent.
Claim 8
Dependent Claim 35 words
The insulated electrical conductor of claim 5, comprising about 10 parts by weight of phosphorylated novolak phenol-formaldehyde and about 1 part by weight of triallyl cyanurate per 100 parts by weight of the ethylene-containing polymer.

References Cited (Backward Citations)

US3124551A Cited
US3119783A Cited
US3149181A Cited
US3376301A Cited
US3297478A Cited
US3367996A Cited
US3331730A Cited
US3527725A Cited
US3644256A Cited
US3697459A Cited
US3752865A Cited
US3817851A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1978-12-29 1979-06-30 1979-12-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1982-12-29 1983-06-30 1983-12-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1986-12-29 1987-06-30 1987-12-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag