Patent US3311842A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3907734A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing powdered polymers

Assignee: Goodyear Tire and Rubber Co
•
Filing: 1973-04-11
•
Granted: 1975-09-23
•
Expires: 1993-04-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of making free-flowing powder from oil and water emulsions by mixing the oil and water emulsion into a partitioning agent containing hydrophobic silica, drying the particulate composition to obtain a powdery plastic or elastomeric composition and in a special embodiment removing at least part of the hydrophobic silica and reusing it to treat further oil and water emulsions.

Inventors

  • 👤 Broeck Theodore R Ten
  • 👤 Raymond E Downey

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 06:26
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/12; C08J3/16; Y; Y10; Y10S; Y10S528/00; Y10S528/931; Y10S528/934

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 55 words
A METHOD OF MAKING A DRY POWDERY PLASTIC OR ELASTOMER COMPOSITION COMPRISING ADDING WITH INTIMATE MIXING A FINE STREAM OF AT LATEX OF A PLASTIC OR ELASTOMER COMPOSITION IN A PARTITIONING AGENT COMPRISED OF A POWDERY HYDROPHOBIC SILICA TO OBTAIN A WET FREE-FLOWING PARTICULATE MASS, AND DRYING THE WET PARTICULATE MASS TO OBTAIN A POWDER..
Claim 2
Independent Claim 55 words
A METHOD OF MAKING A DRY POWDERY PLASTIC OR ELASTOMER COMPOSITION COMPRISING ADDING WITH INTIMATE MIXING A FINE STREAM OF AT LATEX OF A PLASTIC OR ELASTOMER COMPOSITION IN A PARTITIONING AGENT COMPRISED OF A POWDERY HYDROPHOBIC SILICA TO OBTAIN A WET FREE-FLOWING PARTICULATE MASS, AND DRYING THE WET PARTICULATE MASS TO OBTAIN A POWDER..
Claim 3
Dependent Claim 26 words
The method of claim 1 wherein the partition agent is a blend of hydrophobic silica and precipitated silica in the ratio of 15 to 70 percent.
Claim 4
Dependent Claim 20 words
The method of claim 2 wherein at least 90 percent of the hydrophobic silica is recovered from the dry powder.
Claim 5
Dependent Claim 16 words
The method of claim 3 wherein the recovered hydrophobic silica is used to treat more latex.
Claim 6
Dependent Claim 20 words
The method of claim 1 wherein the latex contains an alkali soap of a fatty acid as the emulsifying agent.
Claim 7
Dependent Claim 15 words
The method of claim 5 wherein the alkali soap is a sodium or potassium soap.
Claim 8
Dependent Claim 22 words
The method of claim 1 wherein the plastic or elastomeric composition is a solid over the temperature range of 20* to 50*C.
Claim 9
Dependent Claim 22 words
The method of claim 1 wherein a hundred parts oF latex is used to 4 to 80 parts of hydrophobic silicon dioxide.
Claim 10
Dependent Claim 23 words
The method of claim 1 wherein 5 to 60 percent of precipitated silicon dioxide is used in conjunction with the hydrophobic silicon dioxide.

References Cited (Backward Citations)

US2597892A Cited
US3317446A Cited
US3663655A Cited
US3700619A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1978-09-22 1979-03-24 1979-09-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1982-09-22 1983-03-24 1983-09-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1986-09-22 1987-03-24 1987-09-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag