Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
89 words
A SUBSTITUTE TABACCO MATERIAL COMPRISING A DEGRADED CELLULOSE HAVING AN AVERAGE D.P. OF UP TO 95 AND PREPARED BY TREATING A CELLULOSE WITH AM ALKALI FOLLOWED BY AGING OF THE RESULTING ALKALI CELLULOSE WITH AN OXYGEN-CONTAINING GAS, AND SODIUM CELLULOSE GLYCOLATE IN WHICH THE DEGREE OF SUBSTITUTION OF CARBOXYMETHOXY GROUP IS BETWEEN 0.6 AND 1.0 PERCENT AQUEOUS SOLUTION THEREOF HAS A VISCOSITY OF BETWEEN 80 AND 1,800 CENTIPOISES AT 20*C, THE SAID DEGRADED CELLULOSE BEING CONTAINED THEREIN IN AN AMOUNT AT LEAST 75 PERCENT BY WEIGHT OF SAID MATERIAL.
Claim 2
Dependent Claim
89 words
A SUBSTITUTE TABACCO MATERIAL COMPRISING A DEGRADED CELLULOSE HAVING AN AVERAGE D.P. OF UP TO 95 AND PREPARED BY TREATING A CELLULOSE WITH AM ALKALI FOLLOWED BY AGING OF THE RESULTING ALKALI CELLULOSE WITH AN OXYGEN-CONTAINING GAS, AND SODIUM CELLULOSE GLYCOLATE IN WHICH THE DEGREE OF SUBSTITUTION OF CARBOXYMETHOXY GROUP IS BETWEEN 0.6 AND 1.0 PERCENT AQUEOUS SOLUTION THEREOF HAS A VISCOSITY OF BETWEEN 80 AND 1,800 CENTIPOISES AT 20*C, THE SAID DEGRADED CELLULOSE BEING CONTAINED THEREIN IN AN AMOUNT AT LEAST 75 PERCENT BY WEIGHT OF SAID MATERIAL.
Claim 3
Dependent Claim
79 words
A substitute tobacco material comprising a degraded cellulose having an average D.P. of up to 95 and prepared by treating a cellulose with an alkali followed by aging of the resulting alkali cellulose with an oxygen-containing gas, and hydroxyethyl cellulose, a 2 percent agueous solution of which hydroxyethyl cellulose has a viscosity of between 70 and 4,000 centipoises at 20*C., the said degraded cellulose being contained therein in an amount at least 75 percent by weight of said material.
Claim 4
Dependent Claim
79 words
A substitute tobacco material comprising a degraded cellulose having an average D.P. of up to 95 and prepared by treating a cellulose with an alkali followed by aging of the resulting alkali cellulose with an oxygen-containing gas, and hydroxyethyl cellulose, a 2 percent agueous solution of which hydroxyethyl cellulose has a viscosity of between 70 and 4,000 centipoises at 20*C., the said degraded cellulose being contained therein in an amount at least 75 percent by weight of said material.
Claim 5
Dependent Claim
90 words
A substitute tobacco material comprising a degraded cellulose having an average D.P. of up to 95 and prepared by treating a cellulose with an alkali followed by aging of the resulting alkali cellulose with an oxygen-containing gas, and methylcellulose in which the degree of substitution of methoxyl group is between 1.6 and 2.0 and a 2 percent aqueous solution thereof has a viscosity of between 500 and 6,000 centipoises at 20*C., the said degraded cellulose being contained therein in an amount at least 75 percent by weight of said material.
Claim 6
Dependent Claim
90 words
A substitute tobacco material comprising a degraded cellulose having an average D.P. of up to 95 and prepared by treating a cellulose with an alkali followed by aging of the resulting alkali cellulose with an oxygen-containing gas, and methylcellulose in which the degree of substitution of methoxyl group is between 1.6 and 2.0 and a 2 percent aqueous solution thereof has a viscosity of between 500 and 6,000 centipoises at 20*C., the said degraded cellulose being contained therein in an amount at least 75 percent by weight of said material.
Claim 7
Dependent Claim
73 words
A substitute tobacco material comprising a degraded cellulose having an average D.P. of up to 95 and prepared by treating a cellulose with an alkali followed by aging of the resulting alkali cellulose with an oxygen-containing gas, and ethyl cellulose in which the degree of substitution of ethoxyl group is between 0.6 and 1.5, the said degraded cellulose being contained therein in an amount at least 75 percent by weight of said material.
Claim 8
Dependent Claim
73 words
A substitute tobacco material comprising a degraded cellulose having an average D.P. of up to 95 and prepared by treating a cellulose with an alkali followed by aging of the resulting alkali cellulose with an oxygen-containing gas, and ethyl cellulose in which the degree of substitution of ethoxyl group is between 0.6 and 1.5, the said degraded cellulose being contained therein in an amount at least 75 percent by weight of said material.