Abstract

Abstract A method is provided for making polyetherimides having improved heat stability involving the initial production of a polyetherimide by the nitro-displacement of dinitro-bisimide with alkali diphenoxide and the employment with the resulting polyetherimide of an alkali metal phenoxide stabilizer.

Inventors

  • 👤 D White
  • 👤 F Williams

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 00:05
CPC Classifications
C; C07; C07D; C07D209/00; C07D209/02; C07D209/44; C07D209/48; C08; C08G; C08G73/00; C08G73/06; C08G73/10; C08G73/1003; C08G73/1046; C08G73/1053; C08K; C08K5/00; C08K5/04; C08K5/13

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 38 words
A METHOD FOR STABLIZING POLYETHERIMIDE WHICH COMPRISES HEATING AN ORGANIC SOLVENT SOLUTION OF SAID POLYETHERMIDE CONTAINING AT LEAST 1-10 PERCENT BY WEIGHT BASED ON THE WEIGHT OF SAID POLYETHERIMIDE OF AN ALKALI METAL ORGANIC STABILIZER OF THE FORMULA,
Claim 2
Independent Claim 38 words
A METHOD FOR STABLIZING POLYETHERIMIDE WHICH COMPRISES HEATING AN ORGANIC SOLVENT SOLUTION OF SAID POLYETHERMIDE CONTAINING AT LEAST 1-10 PERCENT BY WEIGHT BASED ON THE WEIGHT OF SAID POLYETHERIMIDE OF AN ALKALI METAL ORGANIC STABILIZER OF THE FORMULA,
Claim 3
Dependent Claim 22 words
A method in accordance with claim 1, which is employed to effect a controlled reduction in the intrinsic viscosity of the polyetherimide.
Claim 4
Dependent Claim 24 words
A method in accordance with claim 1, where the polyetherimide forms no more than 1 percent by weight gel at temperatures up to 315*C.
Claim 5
Dependent Claim 15 words
A method in accordance with claim 1, where the stabilizer is an alkali metal cresoxide.
Claim 6
Dependent Claim 21 words
A method in accordance with claim 1, where polyetherimide is stabilized with about 5 percent by weight of alkali metal phenoxide.
Claim 7
Dependent Claim 30 words
A method in accordance with claim 1, where the polyetherimide is stabilized by heating with alkali metal phenoxide to a temperature of about 60*C for up to about 30 minutes.
Claim 8
Dependent Claim 10 words
A method in accordance with claim 1, where R is
Claim 9
Dependent Claim 10 words
A method in accordance with claim 1, where R1 is
Claim 10
Dependent Claim 10 words
A method in accordance with claim 1, where R1 is
Claim 11
Dependent Claim 15 words
A method in accordance with claim 1, when the alkali metal phenoxide is sodium thiocresoxide.

References Cited (Backward Citations)

US2745882A Cited
US3803103A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-12-16 1978-06-17 1978-12-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-12-16 1982-06-17 1982-12-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1985-12-16 1986-06-17 1986-12-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag