Pavement composition
Assignee: First Interstate Bank of Arizona
•
Filing: 1973-07-20
•
Granted: 1974-10-29
•
Expires: 1993-07-20
Abstract
Abstract An elastomeric paving material that can be applied with conventional equipment. The material is prepared from paving asphalt, asphalt-soluble, non-oil resistant rubbers and an asphalt solvent. The asphalt and rubber are reacted to form a hot thick viscous jellied composition. The hot jellied composition is mixed with 20 percent by volume or less of the asphalt solvent to prepare the elastomeric paving material. The material will maintain a low viscosity for a period of time for workability; then it will rapidly increase its viscosity, independent of solvent loss, and set-up.
Inventors
- 👤 R Winters
- 👤 C Mcdonald
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 13:18
CPC Classifications
E; E01; E01C; E01C7/00; E01C7/08; E01C7/35; E01C7/358; C; C08; C08L; C08L95/00; E01C7/18; E01C7/26; E01C7/265
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
317 words
A METHOD OF REPAIRING PAVEMENT SUBJECT TO FATIGUE CRACKING WHICH COMPRISES THE STEPS OF PREPARING AN ELECTROMERIC MATERIAL COMPRISED OF A REACTION PRODUCT OF PAVING ASPHALT AND NON-OIL RESISTANT, ASPHALT-SOBULBE RUBBER, AND AN ASPHALT SOLVENT, SAID ASPHALT HAVING A PENETRATION GRADE OF ABOUT 10-10 TO ABOUT 200-300, SAID RUBBER BEING AN UNVULCANIZED, VULCANIZED OR RECLAIMED RUBBER SELECTED FROM THE FOLLOWING GROUP: ISOPRENE RUBBER, NATURAL RUBBER, BUTADIENE RUBBER, BUTADIENE-STYRENE RUBBER, BUTYL RUBBER AND ETHYLENE PROPLENE RUBBER; AND THE METHOD COMPRISING HEATING THE ASPHALT TO A FIRST TEMPERATURE BETWEEN ABOUT 300* AND ABOUT 500*F. TO YEILD HOT LIQUID ASPHALT HAVING A VICOSITY OF LESS THAN 200 CENTPOISES; REACTING BETWEEN ABOUT 2 AND ABOUT 4 PARTS, BY WEIGHT, OF THE HOT ASPHALT WITH ONE PART OF THE RUBBER, GRANULATED TO A MESH SIZE BETWEEN -NO. 4 AND +NO. 50, TO FORM A JELLIED-ASPHALT-RUBBER COMPOSITION HAVING A VISCOSITY OF FROM ABOUT 2000 TO ABOUT 200,000 CENTIPOISES; ALLOWING THE JELLIEDASPHALT-RUBBER COMPOSITION TO COOL TO A SECOND TEMPERATURE OF FROM ABOUT 200* TO ABOUT 400*F.; MIXING THE COOLED JELLIEDASPHALT-RUBBER COMPOSITION WITH BETWEEN ABOUT 5 PERCENT AND ABOUT 20 PERCENT BY VOLUME OF THE COMPOSITION OF AN ASPHALT SOLVENT SELECTED FROM THE GROUP CONSISTING OF DEROSENE, ALIPHATIC AND AROMATIC HYDROCARBONS, SOLVENT NAPHTHA, LIGROIN, PAINT THINNER, DIESEL OIL, LIGHT OIL FRACTIONS FROM COAL TAR, WHITE GASOLINE, PETROLEUM SPIRITS, PARAFFINIC OILS, AND HALOGENATED HYDROCARBONS, SAID SOLVENT HAVING A BOILING POINT ABOVE SAID SECOND TEMPERATURE BUT NOT LESS THAN ABOUT 175*F. TO FORM THE ELASTOMERIC MATERIAL HAVING A VISCOSITY OF FROM ABOUT 1000 TO ABOUT 10,000 CENTIPOISES, SAID MATERIAL ADAPTED TO SET UP AND INCREASE ITS VISCOSITY TO A VALUE EQUAL TO THE JELLIED-ASPHALT RUBBER COMPOSITION AFTER A PREDETERMINED PERIOD OF TIME AT SAID SECOND TEMPERATURE WITH LESS THAN ABOUT A 5 PERCENT LOSS OF THE SOLVENT; AND APPLYING A PREDETERMINED AMOUNT OF THE MATERIAL TO THE SURFACE TO BE TREATED AND ALLOWING IT TO SET UP.
Claim 2
Dependent Claim
23 words
The method as defined in claim 1 wherein the asphalt is heated at a first temperature of from about 350* to about 400*F.
Claim 3
Dependent Claim
23 words
The method as defined in claim 1 wherein the mesh size of the rubber is from about -No. 16 to about +No. 25.
Claim 4
Dependent Claim
18 words
The method as defined in claim 1 wherein the second temperature is from about 320* to about 340*F.
Claim 5
Dependent Claim
29 words
The method as defined in claim 1 wherein the asphalt and rubber are reacted by mixing them together for a period of from about 10 to about 90 minutes.
Claim 6
Dependent Claim
27 words
The method as defined in claim 1 wherein the asphalt-rubber-jellied composition is mixed with about 7- 1/2 percent by volume of the composition of the asphalt solvent.
Claim 7
Dependent Claim
13 words
The method as defined in claim 1 wherein the asphalt solvent is kerosene.
Claim 8
Dependent Claim
25 words
The method as defined in claim 1 including the additional steps of covering the applied material with stone aggregate chips before the material sets up.
References Cited (Backward Citations)
US607884A
Cited
US656094A
Cited
US1603502A
Cited
US2310972A
Cited
US2578001A
Cited
US2700655A
Cited
US2861895A
Cited
US3049836A
Cited
US3253521A
Cited
US3270631A
Cited
BE651227A
Cited
US3340780A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1977-10-28 | 1978-04-29 | 1978-10-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1981-10-28 | 1982-04-29 | 1982-10-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1985-10-28 | 1986-04-29 | 1986-10-29 | $7700.00 | Window Closed / Lapsed |