← Back to Patent Explorer
US3816358A Expired / Lapsed US ⏱️ 0.0 years remaining

Vulcanizable rubber mixtures

Assignee: Huels AG
•
Filing: 1972-06-22
•
Granted: 1974-06-11
•
Expires: 1992-06-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Vulcanizable rubber mixtures having improved room temperature hardness containing 2-20% by weight, calculated on the rubber, of a polyoctenamer or polydodecenamer.

Inventors

  • 👤 K Nordsiek
  • 👤 R Streck

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 18:31
CPC Classifications
C; C08; C08L; C08L21/00; C08K; C08K3/00; C08K3/02; C08K3/04; C08K3/06; C08K3/18; C08K3/20; C08K3/22; C08K5/00; C08K5/04; C08K5/09; C08L23/00; C08L23/02; C08L23/16; C08L23/18; C08L23/20; C08L23/22; C08L23/24; C08L65/00; C08L7/00; C08L9/00; C08L9/06; C08L91/00; C08L2312/00; C08L2666/00; C08L2666/02; C08L2666/04; Y; Y10; Y10T; Y10T152/00; Y10T152/10; Y10T152/10495; Y10T152/10765; Y10T152/1081; Y10T152/10819; Y10T152/10846

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 24 words
A vulcanizable elastomeric mixture according to claim 1 containing 5-15 percent of a polyoctenamer having double bonds which are 75-95 percent in the trans-configuration.
Claim 2
Dependent Claim 24 words
A vulcanizable elastomeric mixture according to claim 1 containing 5-15 percent of a polydodecenamer having double bonds which are 75-95 percent in the trans-configuration.
Claim 3
Dependent Claim 26 words
A vulcanizable elastomeric mixture according to claim 1 wherein the elastomer is selected from the group consisting of natural rubber, polyisoprene, styrene-butadiene rubber and cis-1, 4-polybutadiene.
Claim 4
Dependent Claim 34 words
A vulcanizable elastomeric mixture according to claim 1 having a deformation hardness at 20* of more than 4,000, wherein the elastomer therein has a deformation hardness of from 2,000 to 4,000 at 20* C.
Claim 5
Dependent Claim 36 words
A vulcanizable elaStomeric mixture according to claim 1 having a deformation hardness at 20* C. of from 5,000 to 9,000, wherein the elastomer therein has a deformation hardness of from 2,000 to 4,000 at 20* C.
Claim 6
Dependent Claim 22 words
A cross-linked vulcanizate of the elastomeric mixture according to claim 5, having a deformation hardness at 20* C. of more than 4,000.
Claim 7
Independent Claim 95 words
A method of increasing the deformation hardness of a vulcanizable elastomeric mixture whose elastomer has a deformation hardness at 20* C. of less than 6,000, which comprises incorporating therein an amount from 2-20 percent by weight, based on the elastomer, effective to impart a deformation hardness to the elastomeric mixture which is substantially greater than the deformation hardness of the elastomer, of a polyoctenamer, a polydodecenamer or a mixture thereof, whose double bonds are more than 60 percent in the trans-configuration and which has a reduced viscosity of 0.2 - 3.0 dl./g. at 135* C.
Claim 8
Dependent Claim 22 words
A method according to claim 8 wherein a polyoctenamer having double bonds which are 75-95 percent in the trans-configuration is incorporated therein.
Claim 9
Dependent Claim 22 words
A method according to claim 8 wherein a polydodecenamer having double bonds which are 75-95 percent in the trans-configuration is incorporated therein.
Claim 10
Dependent Claim 19 words
A method according to claim 8 wherein 5-15 percent of the polyoctenamer, polydodecenamer or mixture thereof is incorporated therein.
Claim 11
Dependent Claim 23 words
A method according to claim 8 wherein the elastomer is selected from the group consisting of natural rubber, polyisoprene, styrene-butadiene rubber and cis-1,4-polybutadiene.
Claim 12
Dependent Claim 18 words
An article of manufacture comprising an unvulcanized automobile tire formed of an elastomeric mixture according to claim 5.
Claim 13
Dependent Claim 18 words
An article of manufacture comprising an unvulcanized automobile tire formed of an elastomeric mixture according to claim 6.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-06-10 1977-12-10 1978-06-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-06-10 1981-12-10 1982-06-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1985-06-10 1985-12-10 1986-06-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag