Abstract

Abstract A more uniform cladding thickness is retained on flat copperclad steel wire by drawing the first rectangular sections, rather than rolling them, from round wire, and then rolling the final flat wire.

Inventors

  • 👤 A Barone
  • 👤 Ascoli R D
  • 👤 C Bechle

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 08:36
CPC Classifications
B; B21; B21C; B21C37/00; B21C37/04; B21C37/042; B23; B23K; B23K20/00; Y; Y10; Y10S; Y10S72/00; Y10S72/70

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 57 words
The method of forming a flat copper-clad steel wire comprising the steps of: A. cold dRawing round copper-clad steel wire into a wire of rectangular section, and B. cold rolling said rectangular sectioned wire thereby flattening the same and decreasing its sectional area while retaining a substantial thickness of copper over the entire surface of said wire.
Claim 2
Independent Claim 57 words
The method of forming a flat copper-clad steel wire comprising the steps of: A. cold dRawing round copper-clad steel wire into a wire of rectangular section, and B. cold rolling said rectangular sectioned wire thereby flattening the same and decreasing its sectional area while retaining a substantial thickness of copper over the entire surface of said wire.
Claim 3
Dependent Claim 27 words
The method of claim 1 wherein the longer dimension of a section of said flattened wire is at least four times the shorter dimension of said section.
Claim 4
Dependent Claim 29 words
The method of claim 2 wherein the longer dimension of said rectangular section after drawing but prior to rolling is at least twice the shorter dimension of said section.
Claim 5
Dependent Claim 24 words
The method of claim 1 wherein said cold drawing into a rectangular section is effected through a plurality of dies in a continuous run.
Claim 6
Dependent Claim 24 words
The method of claim 3 wherein said cold drawing into a rectangular section is effected through a plurality of dies in a continuous run.
Claim 7
Dependent Claim 26 words
The method of claim 2 wherein said longer dimension exceeds the longer dimension of the final of said rectangular sections after drawing but prior to rolling.

References Cited (Backward Citations)

US1813539A Cited
US1922770A Cited
US2152842A Cited
US2134014A Cited
US2146788A Cited
US2268617A Cited
US2286759A Cited
US3645123A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-05-20 1977-11-19 1978-05-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-05-20 1981-11-19 1982-05-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1985-05-20 1985-11-19 1986-05-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag