Abstract

Abstract A low alloy steel which utilizes boron as an essential alloying ingredient. The boron controls and manipulates the fragment mass distribution characteristics of alloy steels used in fabricating explosive warheads.

Inventors

  • 👤 T Watmough
  • 👤 Shea R O

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 23:33
CPC Classifications
C; C22; C22C; C22C38/00; C22C38/18; C22C38/24; C22C38/002

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 12 words
An alloy in accordance with claim 1 containing about 0.002 percent boron.
Claim 2
Dependent Claim 12 words
An alloy in accordance with claim 1 containing about 0.006 percent boron.

References Cited (Backward Citations)

US2528867A Cited
US2683086A Cited
US2737455A Cited
US2858206A Cited
US3288600A Cited
US3615879A Cited
US3547032A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-02-11 1977-08-13 1978-02-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-02-11 1981-08-13 1982-02-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1985-02-11 1985-08-13 1986-02-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag