← Back to Patent Explorer
US3783125A Expired / Lapsed US ⏱️ 0.0 years remaining

Sweetening liquid hydrocarbons with a calcined heavy metal exchanged zeolite

Assignee: Howe Baker Engineers LLC
•
Filing: 1972-09-21
•
Granted: 1974-01-01
•
Expires: 1992-09-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract 1. A LIQUID HYDROCARBON CONTAINING ORGANIC MERCAPTANS IS CONTACTED WITH A HEAVY METAL EXCHANGED ALUMINOSILICATE ZEOLITE CONTAINING FROM 5 TO 20% BY WEIGHT OF COPPER, CHROMIUM, TIN OR MIXTURES THEREOF TO CONVERT THE MERCAPTANS TO DISULFIDES. THE METAL EXCHANGE ZEOLITE IS PREPARED FROM A DILUTE SOLUTION OF THE METAL SALT, RINSED, DRIED AT 80-150*C. FOR 2-6 HOURS, HEATED TO 500*C. FOR 4-8 HOURS, CALCINED AT 500-700*C. FOR 6-12 HOURS AND THEN COOLED OVER A PERIOD OF 3-6 HOURS.

Inventors

  • 👤 J Ondrey
  • 👤 M Basila

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 16:13
CPC Classifications
C; C10; C10G; C10G17/00; C10G17/095; B; B01; B01J; B01J20/00; B01J20/02; B01J20/10; B01J20/16; B01J20/18; B01J20/186; B01J29/00; B01J29/04; B01J29/06; B01J29/061; B01J37/00; B01J37/08; C10G25/00; C10G25/02; C10G25/03; C10G25/05; C10G27/00; C10G27/04; C10G29/00

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 77 words
A LIQUID HYDROCARBON CONTAINING ORGANIC MERCAPTANS IS CONTACTED WITH A HEAVY METAL EXCHANGED ALUMINOSILICATE ZEOLITE CONTAINING FROM 5 TO 20% BY WEIGHT OF COPPER, CHROMIUM, TIN OR MIXTURES THEREOF TO CONVERT THE MERCAPTANS TO DISULFIDES. THE METAL EXCHANGE ZEOLITE IS PREPARED FROM A DILUTE SOLUTION OF THE METAL SALT, RINSED, DRIED AT 80-150*C. FOR 2-6 HOURS, HEATED TO 500*C. FOR 4-8 HOURS, CALCINED AT 500-700*C. FOR 6-12 HOURS AND THEN COOLED OVER A PERIOD OF 3-6 HOURS.
Claim 2
Dependent Claim 77 words
A LIQUID HYDROCARBON CONTAINING ORGANIC MERCAPTANS IS CONTACTED WITH A HEAVY METAL EXCHANGED ALUMINOSILICATE ZEOLITE CONTAINING FROM 5 TO 20% BY WEIGHT OF COPPER, CHROMIUM, TIN OR MIXTURES THEREOF TO CONVERT THE MERCAPTANS TO DISULFIDES. THE METAL EXCHANGE ZEOLITE IS PREPARED FROM A DILUTE SOLUTION OF THE METAL SALT, RINSED, DRIED AT 80-150*C. FOR 2-6 HOURS, HEATED TO 500*C. FOR 4-8 HOURS, CALCINED AT 500-700*C. FOR 6-12 HOURS AND THEN COOLED OVER A PERIOD OF 3-6 HOURS.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1976-12-31 1977-07-02 1978-01-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1980-12-31 1981-07-02 1982-01-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1984-12-31 1985-07-02 1986-01-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag