Method of manufacturing fine grain ceramic barium titanate

Assignee: Panasonic Holdings Corp
•
Filing: 1972-02-17
•
Granted: 1973-10-09
•
Expires: 1992-02-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of manufacturing fine grain barium titanate ceramic bodies from compositions including semiconducting barium titanate ordinarily doped with Nb2O5, Ta2O5, Sb2O5, Bi2O3, La2O3, CeO2, Gd2O3, Sm2O3, and Y2O3, and dielectric barium titanate. Barium sulfate is included as a starting ingredient in the barium titanate materials, and the materials are calcined and fired in a conventional manner. The resulting ceramic materials have uniform fine grain size.

Inventors

  • 👤 S Hayakawa
  • 👤 Y Matsuo
  • 👤 H Sasaki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 23:40
CPC Classifications
H; H01; H01C; H01C7/00; H01C7/04; H01C7/042; H01C7/043; H01C7/045; C; C04; C04B; C04B35/00; C04B35/01; C04B35/46; C04B35/462; C04B35/465; C04B35/468; C04B35/4682; C04B35/4684

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 49 words
A method as claimed in claim 1 wherein said primary mixture has a composition, consisting essentially of 99.5 to 99.995 weight % of BaTiO3 and 0.005 to 0.5 weight % of one oxide selected from the group consisting of Nb2O5, Ta2O5, Sb2O3, Bi2O3, La2O3, CeO2, Gd2O3, Sm2O3 and Y2O3.
Claim 2
Dependent Claim 31 words
A method as claimed in claim 2 wherein said primary mixture is calcined at a temperature of 1000 to 1200*C and then admixed with 0.05 to 2.00 weight % of BaSO4.
Claim 3
Dependent Claim 35 words
A method as claimed in claim 1 wherein said composition has 1 to 35 atom % of Ba replaced by an equivalent amount of one element selected from the group consisting of Sr and Pb.
Claim 4
Dependent Claim 35 words
A method as claimed in claim 1 wherein said composition has 1 to 20 atom % of Ti replaced by an equivalent amount of one element selected from the group consisting of Sn and Zr.

References Cited (Backward Citations)

US3028248A Cited
US3673119A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1976-10-08 1977-04-09 1977-10-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1980-10-08 1981-04-09 1981-10-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1984-10-08 1985-04-09 1985-10-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag