US3753748A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Hydraulic cement retarder composition
Assignee: Schlumberger Technology Corp
•
Filing: 1971-12-23
•
Granted: 1973-08-21
•
Expires: 1991-12-23
Abstract
Abstract In a method of cementing at relatively high ambient temperatures employing an aqueous hydraulic cement slurry, the improvement comprising admixing therewith an effective amount of both (1) a salt of lignosulfonic acid and (2) boric acid or a borate whereby a synergistic retarding effect on the setting rate of the slurry is attained without any accompanying adverse effects.
Inventors
- 👤 R Martin
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 10:48
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/42; C09K8/46; C04; C04B; C04B28/00; C04B28/02
Claims Analysis
Total Claims: 0
No claims parsed yet. Click Sync Now above to re-index claims from Google Patents.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1976-08-20 | 1977-02-19 | 1977-08-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1980-08-20 | 1981-02-19 | 1981-08-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1984-08-20 | 1985-02-19 | 1985-08-21 | $7700.00 | Window Closed / Lapsed |