Abstract

Abstract A METHOD OF IMPROVING THE PROPERTIES OF HEAT HARDENABLE COPPER ALLOYS BY HEATING THE ALLOY IN ITS ORIGINAL CAST FORM TO ITS SOLUTION ANNEALING TEMPERATURE, WORKING THE HEATED ALLOY TO A SELECTED SEMI-FINISHED CROSS SECTION AND IMMEDIATELY THEREAFTER QUENCHING THE ALLOY IN ITS WORKED FORM TO THEREBY OBTAIN A FINE GRAIN STRUCTURE GIVING RISE TO IMPROVED MECHANICAL AND ELECTRICAL PROPERTIES.

Inventors

  • 👤 H Wallbaum

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 10:06
CPC Classifications
H; H01; H01B; H01B1/00; H01B1/02; H01B1/026; C; C22; C22C; C22C9/00; C22F; C22F1/00; C22F1/08

Claims Analysis

Total Claims: 0
No claims parsed yet. Click Sync Now above to re-index claims from Google Patents.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1976-02-20 1976-08-21 1977-02-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1980-02-20 1980-08-21 1981-02-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1984-02-20 1984-08-21 1985-02-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag