Fast warm-up indirectly heated cathode structure
Abstract
Abstract A tungsten heater, covered with a thin alumina layer (about 1 mil), is potted inside a molybdenum cathode cup in a sintered mass formed from a mixture of fine particles (of the order of 1-5 microns) of molybdenum and nickel in the weight ratio of at least 40 percent molybdenum, but preferably about 90 percent moly. The emissive surface of the cup has a matrix of sintered nickel carbonyl filled with alkaline earth metal emissive oxides. The cup is supported by invar struts. The processing includes: (1) preparing a sintered nickel carbonyl matrix layer for the emissive surface of the cup; (2) ball-milling molybdenum-nickel mix with butyl carbitol, and after covering the heater therewith, inserting the heater in the cup, firing the assembly in hydrogen at between 1,150* to 1,350* C until sintered; and (3) impregnating the nickel carbonyl matrix with a mix of alkaline earth carbonates in methyl alcohol and using heat and ultrasonic vibration to compete impregnation. After assembly in tubes, activation and aging follows.
Inventors
- 👤 Clayton L Waltermire
Bibliographic Details
Claims Analysis
Total Claims: 7References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1975-06-20 | 1975-12-20 | 1976-06-20 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1979-06-20 | 1979-12-20 | 1980-06-20 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1983-06-20 | 1983-12-20 | 1984-06-20 | $7700.00 | Window Closed / Lapsed |