Piezoelectric structure composed of a ceramic ferro-electric material having a perovskite arrangement of components
Abstract
Abstract WHEREIN X, Y AND Z ARE NUMERALS THE SUM OF WHICH IS EQUAL TO 1. THE FERRO-ELECTRIC MATERIALS ALSO INCLUDES ABOUT 1% OF MNO2 AND 0.15% AL2O3 BY WEIGHT OF ALL OF THE COMPONENTS. THE DISCLOSED STRUCTURE HAS AN IMPROVED ELECTRO-MECHANICAL COUPLING FACTOR K, AN IMPROVED MECHANICAL QUALITY FACTOR Q AND AN INCREASED DIELECTRIC EVALUE FACTOR, ALL OF WHICH FACTORS ARE SELECTIVELY ADJUSTABLE BY SELECTION OF INDIVIDUAL COMPONENTS AND THEIR AMOUNTS. XPBTIO3-YPBZRO3-2PB(MG0.5W0.5)O3 A PIECOELECTRIC STRUCTURE COMPRISED OF A CERAMIC FEROELECTRIC MATERIAL HAVING A PEROVSKITE ARRANGEMENT OF COMPONENTS DEFINED BY THE GENERAL FORMULA: 41 THROUGH 49 MOL PERCENT PBTIO3, 37 THROUGH 49 MOL PERCENT PBZRO3 AND 5 THROUGH 18 MOL PERCENT PB(ANBMO3, WHEREIN A AND B ARE BOTH INDIVIDUAL AND DISTINCT CHEMICAL ELEMENTS, EACH HAVING A POSITIVE VALENCE AND N AND M ARE POSITIVE NUMERALS, THE SUM OF WHICH EQUALS 1 AND THE SUM OF THE PRODUCT OF THE VALANCE AXN PLUS THE PRODUCT OF THE VALENCE OF BXM IS EQUAL TO 4. FOR EXAMPLE, A PERFERED PEROVSKITE ARRANGEMENT FOR A PREFERRED FERROELECTRIC MATERIAL IS
Inventors
- 👤 Helmut Thomann
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1975-05-16 | 1975-11-15 | 1976-05-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1979-05-16 | 1979-11-15 | 1980-05-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1983-05-16 | 1983-11-15 | 1984-05-16 | $7700.00 | Window Closed / Lapsed |