Antistatic polyamide fiber containing polyether
Abstract
Abstract IT HAS BEEN FOUND THAT AN ANTISTATIC FIBER OF POLYAMIDE, POLYESTER, POLYUREA, POLYURETHANE OR POLYSULFONAMIDE CAN BE PREPARED BY UNIFORMLY DISPERSING BETWEEN ABOUT 1 PERCENT AND ABOUT 12 PERCENT BY WEIGHT OF A COMPOUND REPRESENTED BY THE FORMULA: H-(O-CH2-CH2)Y-(O-CH(-CH3)-CH2)C-N(-CH2-CH(-CH3)-O)D-(CH2- CH2-O)Z-H)-CH2-CH2-N(-(CH2-CH(-CH3)-O)A-(CH2-CH2-O)X-H)- (CH2-CH(-CH3)-O)B-(CH2-CH2-O)W-H WHERE A,B,C,D,W,X,Y, AND Z ARE EACH A WHOLE NUMBER AND THE TOTAL OF A,B,C, AND D IS BETWEEN 8 AND 850 AND THE TOTAL OF W,X,Y, AND Z IS BETWEEN 8 AND 1,000. THE COMPOUND HAS A MOLECULAR WEIGHT BETWEEN ABOUT 4,000 AND 135,000 AND THE ETHYLENE OXIDE MOIETY MAKES UP 10 TO 90% OF THE MOLECULAR WEIGHT OF THE COMPOUND.
Inventors
- 👤 Gene C Weedon
- 👤 Lamberto Crescentini
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1975-04-18 | 1975-10-18 | 1976-04-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1979-04-18 | 1979-10-18 | 1980-04-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1983-04-18 | 1983-10-18 | 1984-04-18 | $7700.00 | Window Closed / Lapsed |