Abstract
Abstract Encapsulated ferrite magnetic memory cores are disclosed which have a very thin coating of polymerized gammaaminopropyltriethoxysilane, whereby the cores are organophilic for adhesion to an uncured silicone rubber-coated substrate, are lubricated to minimize friction with wires passed through the holes in the cores, and are hydrophobic to provide moisturerepellence of the cores in use in a memory. The cores are encapsulated by shaking a substantial bulk quantity of sintered ferrite memory cores in silane vapor at a temperature of about 220* C. in an inert gaseous environment having a known moisture content.
Inventors
- 👤 Thomas Philip Fulton
- 👤 Henry Di Luca
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-29 14:23
CPC Classifications
H; H01; H01F; H01F41/00; H01F41/02; H01F41/0253; H01F41/026; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31652; Y10T428/31663
Claims Analysis
Total Claims: 1
Claim 1
Independent Claim
204 words
The method of encapsulating ferrite magnetic cores, comprising the steps of: loading a measure quantity, such as 10 cc., of gamma-aminopropyltriethoxysilane liquid in a first container, loading a substantial bulk quantity, such as two million, of ferrite magnetic cores in a second container having a perforate bottom positioned over said first container and having a top opening for the exhaust of fumes, heating said silane liquid in said first container to a temperature of about 220* C. to vaporize the silane liquid, introducing an inert gas, such as nitrogen, having a known moisture content into said first container for passage with said vapor through said second container to provide a reaction environment containing a known moisture content, whereby the silane vapor polymerizes on the surfaces of the cores due to a chemical reaction involving moisture on the core surfaces and in the gaseous environment, and vibrating said cores in said first container to fully expose all surfaces of the cores to said silane vapor and to prevent the cores from sticking to each other, said treatment of the cores being continued for about 10 minutes or until the core surfaces are primed to a thickness of about a few hundred molecules of polymerized silane.
References Cited (Backward Citations)
US2306222A
Cited
US2730841A
Cited
US2993809A
Cited
US3279945A
Cited
US3445326A
Cited
US3442690A
Cited
US3484333A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1975-02-07 | 1975-08-09 | 1976-02-08 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1979-02-07 | 1979-08-09 | 1980-02-08 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1983-02-07 | 1983-08-09 | 1984-02-08 | $7700.00 | Window Closed / Lapsed |