Abstract

Abstract ted with corona discharge to effect adhesion of differently sensitized photographic silver halide emulsion layers to the polymer surface, the improvement for obtaining greater uniformity of coating and stability of the emulsion layers, comprising activating the polymeric surface with a corona discharge producing a surface tending to fog a silver halide emulsion layer immediately coated thereon, and at least about 30 minutes later but before the adhesive property of the polymeric surface has substantially decreased, coating at least one of the emulsion layers on the activated polymeric surface.

Inventors

  • 👤 Donald B Thomas
  • 👤 Richard W Wheeler
  • 👤 Donald N Miller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 08:29
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/76; G03C1/91; G03C1/915; G03C1/775; G03C1/79

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 30 words
The process of claim 1 wherein the support is paper having polymeric surfaces on each side and the emulsion layers are gelatin-silver halide emulsion layers which contain color-forming coupler compounds.
Claim 2
Dependent Claim 19 words
The process of claim 2 wherein the polymeric surface on at least one side of the paper is polyethylene.
Claim 3
Dependent Claim 27 words
The process of claim 2 wherein the polymeric surface on at least one surface of the paper is polyethylene, polypropylene, an ethylene copolymer or a linear polyester.
Claim 4
Dependent Claim 18 words
The process of claim 2 wherein the emulsion layers are coated simultaneously onto the corona activated polymer surface.
Claim 5
Dependent Claim 38 words
The process of claim 2 wherein one of the emulsion layers is coated just after corona activation of the polymer surface and the remaining emulsion layers are coated thereon at least about 30 minutes after the corona activation.
Claim 6
Dependent Claim 15 words
The process of claim 1 wherein the sensitive layer is a gelatin-silver halide emulsion layer.
Claim 7
Dependent Claim 8 words
The light-sensitive element prepared according to claim 2.
Claim 8
Dependent Claim 8 words
The light-sensitive element prepared according to claim 5.
Claim 9
Dependent Claim 8 words
The light-sensitive element prepared according to claim 6.
Claim 10
Dependent Claim 19 words
The process of claim 1 wherein the current frequency of the corona discharge is greater than about 200 Hz.

References Cited (Backward Citations)

US3222176A Cited
US3117865A Cited
US3266895A Cited
US3411908A Cited
US3411910A Cited
FR1460174A Cited
GB1134211A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1974-09-20 1975-03-22 1975-09-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1978-09-20 1979-03-22 1979-09-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1982-09-20 1983-03-22 1983-09-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag