Abstract

Abstract An electrical alloy which is essentially free of cobalt and carbon and comprising, as expressed in percent by weight: NICKEL: 40-46%; MANGANESE: 2.5-3.5%; IRON: 0.5-0.6% COPPER-BALANCE

Inventors

  • 👤 Arnold J Gottlieb
  • 👤 Teh Po Wang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 04:31
CPC Classifications
H; H01; H01B; H01B1/00; H01B1/02; H01B1/026; C; C22; C22C; C22C9/00; C22C9/06

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 14 words
An alloy as set forth in claim 1 wherein the carbon content 0.005 percent.
Claim 2
Dependent Claim 14 words
An alloy as set forth in claim 2 wherein the cobalt content 0.03 percent.
Claim 3
Dependent Claim 16 words
An alloy as set forth in claim 3 containing: 43% nickel; 3% manganese; 0.25% iron; balance-copper

References Cited (Backward Citations)

US2224573A Cited
US2696544A Cited
US3017269A Cited
US3266891A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1974-09-20 1975-03-22 1975-09-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1978-09-20 1979-03-22 1979-09-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1982-09-20 1983-03-22 1983-09-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag