← Back to Patent Explorer
US3607150A Expired / Lapsed US ⏱️ 0.0 years remaining

Gold-filled metal for jewelry manufacture

Assignee: ROBERT P BEEKMAN
•
Filing: 1968-12-30
•
Granted: 1971-09-21
•
Expires: 1988-12-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A nickel alloy base layer, consisting substantially of copper 65 percent, nickel in the range of 10 to 18 percent and the balance zinc, has a thin, substantially pure nickel backing bonded on one side. On the other side is carried a layer of gold of suitable karat, with or without the interposition of another thinner layer of substantially pure nickel bonded between the base and to the gold to form an interliner. The interliner is used when the nickel alloy consists of nickel substantially in the range of 10 to 14 percent. The interliner is omitted when the nickel alloy consists of nickel substantially in the range of 15 to 18 percent. Bonding is performed in the solid phase by rolling.

Inventors

  • 👤 Thomas E Mcginn

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 23:02
CPC Classifications
B; B32; B32B; B32B15/00; B32B15/01; B32B15/018; B23; B23K; B23K20/00; B23K20/04; Y; Y10; Y10S; Y10S428/00; Y10S428/922; Y10S428/923; Y10S428/924; Y10S428/926; Y10T; Y10T428/00; Y10T428/12; Y10T428/12493; Y10T428/12771; Y10T428/12861; Y10T428/12889; Y10T428/12903; Y10T428/1291

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 42 words
A composite according to claim 1 wherein the total thickness of the composite is in the range of approximately 0.008 inch to 0.012 inch, and the minimum thicknesses of the nickel backing layer and of the gold layer are approximately 0.001 inch.
Claim 2
Dependent Claim 71 words
Composite gold-filled metal, comprising an alloy base which consists of nickel in the range of approximately 10 to 14 percent, copper on the order of 65 percent and the balance zinc, a substantially pure nickel backing bonded to one side of said base, a layer of gold on the other side of the base and a substantially pure nickel interliner between the base and the gold layer are bonded to each.
Claim 3
Dependent Claim 49 words
Gold-filled metal according to claim 3 wherein the total thickness of the composite is in the range of 0.008 inch to 0.012 inch, the minimum thicknesses of the nickel backing and gold facing are approximately 0.001 inch and the minimum thickness of said nickel interliner is approximately 0.001 inch.
Claim 4
Dependent Claim 52 words
Composite gold-filled metal, comprising an alloy base which consists of nickel in the range of approximately 15 to 18 percent, copper 65 percent and the balance zinc, a substantially pure nickel backing bonded on one side of said base, and a layer of gold bonded to the other side of the base.
Claim 5
Dependent Claim 40 words
Gold-filled metal according to claim 5 wherein the total thickness of the composite is approximately in the range of 0.008 inch to 0.012 inch, and the minimum thickness of the nickel-backing layer and of the gold layer are 0.001 inch.

References Cited (Backward Citations)

US2120561A Cited
US3000085A Cited
US3221219A Cited
US3367754A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1974-09-20 1975-03-22 1975-09-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1978-09-20 1979-03-22 1979-09-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1982-09-20 1983-03-22 1983-09-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag