← Back to Patent Explorer
US3597829A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of making a nickel hydroxide electrode

Assignee: United States Department of the Army
•
Filing: 1969-03-18
•
Granted: 1971-08-10
•
Expires: 1989-03-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A nickel hydroxide electrode suitable for use in an alkaline nickel battery is made by pasting a solvent dispersion of nickel hydroxide onto a nickel foam matrix, drying the pasted matrix, pressing the dried pasted matrix to the required size, and attaching an electrically conductive tab to the electrode.

Inventors

  • 👤 Otto C Wagner
  • 👤 Martin J Sulkes

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 11:05
CPC Classifications
H; H01; H01M; H01M4/00; H01M4/02; H01M4/24; H01M4/32; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y10; Y10T; Y10T29/00; Y10T29/40; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49174

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 14 words
A method to claim 1 wherein conductive carbon is mixed with the nickel hydroxide.
Claim 2
Dependent Claim 8 words
spreading the paste onto a nickel foam matrix,
Claim 3
Dependent Claim 8 words
spreading the paste onto a nickel foam matrix,
Claim 4
Dependent Claim 14 words
drying the pasted matrix at a temperature above the boiling temperature of the solvent,
Claim 5
Dependent Claim 11 words
A method according to claim 1 wherein toluene is the solvent.
Claim 6
Dependent Claim 11 words
drying the pasted matrix at about 80* to about 120* C.,
Claim 7
Dependent Claim 34 words
pressing the dried pasted matrix under a pressure of about one-half ton to about 2 tons per square inch so that the porosity of the finished electrode is about 40 to 60 percent, and
Claim 8
Independent Claim 12 words
A method of making a nickel hydroxide electrode including the steps of:
Claim 9
Dependent Claim 9 words
pressing the dried pasted matrix to electrode size, and
Claim 10
Dependent Claim 8 words
attaching an electrically conductive tab to the electrode.
Claim 11
Dependent Claim 13 words
attaching an electrically conductive tab to the compressed upper corner of the electrode.

References Cited (Backward Citations)

US2895819A Cited
US3009979A Cited
US3024296A Cited
US3184339A Cited
US3436267A Cited
US3393096A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1974-08-09 1975-02-08 1975-08-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1978-08-09 1979-02-08 1979-08-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1982-08-09 1983-02-08 1983-08-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag