Abstract
Abstract AN IMPROVED PROCESS FOR PRODUCING POLYAMINESULFONES WHICH COMPRISES IRRADIATING AN EQUIMOLAR OR SUBSTANTIALLY EQUIMOLAR MIXTURE OF A DIALLYLAMINE DERIVATIVE AND SULFUR DIOXIDE WITH A LIGHT CONTAINING RAYS HAVING A WAVE LENGTH OF 300 TO 450 MU TO BULK-PHOTOCOPOLYMERIZE THE MIXTURE. ACCORDING TO THIS PROCESS, POLYAMINESULFONES CAN EASILY BE OBTAINED IN HIGH YIELDS. SINCE THE ABOVE-MENTIONED MIXTURE IS A HEAT-STABLE, VISCOUS LIQUID, IT CAN BE CONTINUOUSLY EXTRUDED THROUGH A SLIT OR NOZZLE IN THE FORM OF A FILM OR SHEET ANC CAN BE CONTINUOUSLY POLYMERIZED BY CONTINUOUS APPLICATION OF THE ABOVE-MENTIONED LIGHT. AS THE SAID LIGHT, THERE MAY USUALLY BE USED SUNLIGHT OR THE LIGHT FROM A FLUORESCENT LAMP. THE IRRADIATION OF LIGHT IS EFFECTED AT A TEMPERATURE RANGING FROM -100*C. TO 100*C., PREFERABLY FROM - 50*C. TO 50*C.
Inventors
- 👤 Susumu Harada
- 👤 Kunio Arai
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1974-06-14 | 1974-12-14 | 1975-06-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1978-06-14 | 1978-12-14 | 1979-06-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1982-06-14 | 1982-12-14 | 1983-06-15 | $7700.00 | Window Closed / Lapsed |