Abstract

Abstract A process of machining metal castings to minimize warping, especially useful in manufacturing propellers. When the casting is mounted for machining its shallow parts are restrained from warping out of alignment. After machining and while still so restrained, the more critical portions, for example, those near the roots of propeller blades, are machined to contour, then shot peened. The peening hardens the machined surface, increasing its bending resistance, to minimize warping when the casting is released from restraint.

Inventors

  • 👤 John T Parsons

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 02:20
CPC Classifications
B; B23; B23Q; B23Q3/00; B23Q3/02; B23Q3/06; B23Q3/062; B23Q2703/00; B23Q2703/02; B23Q2703/10; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49316; Y10T29/49332; Y10T29/4998; Y10T29/49988; Y10T29/49989; Y10T29/49995; Y10T29/49996

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 99 words
For purpose of minimizing warping, the process of machining a metal casting at least part of which has a cross section defined by an outer surface comprised principally of two opposed surfaces spaced more closely than their width, comprising the steps of: mounting the casting aligned in position for machining and restraining it from warping out of such alignment, then machining at least a portion of said opposed surfaces, and peening at least a portion of the surfaces so machined, whereby to increase the bending resistance of the peened surface portion; and then releasing the casting from such restraint.
Claim 2
Dependent Claim 99 words
For purpose of minimizing warping, the process of machining a metal casting at least part of which has a cross section defined by an outer surface comprised principally of two opposed surfaces spaced more closely than their width, comprising the steps of: mounting the casting aligned in position for machining and restraining it from warping out of such alignment, then machining at least a portion of said opposed surfaces, and peening at least a portion of the surfaces so machined, whereby to increase the bending resistance of the peened surface portion; and then releasing the casting from such restraint.
Claim 3
Dependent Claim 21 words
The process defined in claim 1, wherein the step of peening is performed by propelling shot against such machined surface portion.
Claim 4
Dependent Claim 175 words
For purpose of minimizing warping, the process of machining a metal casting at least part of which has a cross section defined by an outer surface comprised principally of two opposed surfaces spaced more closely than their width, comprising the steps of: mounting the casting aligned in position for machinIng one of said opposed surfaces, and restraining it from warping out of such alignment, and then, while maintaining such restraint against warping; machining at least a portion of one of said opposed surfaces, and peening at least a portion of the surface so machined, then mounting the casting aligned in position for machining the other of said opposed surfaces and restraining it from warping out of such alignment, and then while maintaining such restraint against warping; machining at least a portion of the other of said opposed surfaces and peening at least a portion of such machined surface, whereby increased bending resistance at the peened surface portion compensates in part for the removal by machining of compressed metal at the outer surface of the casting.
Claim 5
Dependent Claim 175 words
For purpose of minimizing warping, the process of machining a metal casting at least part of which has a cross section defined by an outer surface comprised principally of two opposed surfaces spaced more closely than their width, comprising the steps of: mounting the casting aligned in position for machinIng one of said opposed surfaces, and restraining it from warping out of such alignment, and then, while maintaining such restraint against warping; machining at least a portion of one of said opposed surfaces, and peening at least a portion of the surface so machined, then mounting the casting aligned in position for machining the other of said opposed surfaces and restraining it from warping out of such alignment, and then while maintaining such restraint against warping; machining at least a portion of the other of said opposed surfaces and peening at least a portion of such machined surface, whereby increased bending resistance at the peened surface portion compensates in part for the removal by machining of compressed metal at the outer surface of the casting.
Claim 6
Dependent Claim 122 words
The process of machining metal propeller castings, comprising the steps of: mounting the casting by its hub portion in position for machining one set of its blade surfaces and securing its blade portions in desired alignment therewith; machining said set of blade surfaces at and outboard of the root junctures of the blade portions; peening the surfaces so machined, releasing the casting from such restraint; then mounting the casting alignment in position for machining the other set of its blade surfaces and restraining its blade portions in the same desired alignment therewith; machining said other set of blade surfaces at and outboard of the root junctures of the blade portions; peening the surfaces so machined; and releasing the casting from such restraint.
Claim 7
Dependent Claim 122 words
The process of machining metal propeller castings, comprising the steps of: mounting the casting by its hub portion in position for machining one set of its blade surfaces and securing its blade portions in desired alignment therewith; machining said set of blade surfaces at and outboard of the root junctures of the blade portions; peening the surfaces so machined, releasing the casting from such restraint; then mounting the casting alignment in position for machining the other set of its blade surfaces and restraining its blade portions in the same desired alignment therewith; machining said other set of blade surfaces at and outboard of the root junctures of the blade portions; peening the surfaces so machined; and releasing the casting from such restraint.

References Cited (Backward Citations)

US3002266A Cited
US3130481A Cited
US3295190A Cited
US3345727A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1974-04-26 1974-10-26 1975-04-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1978-04-26 1978-10-26 1979-04-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1982-04-26 1982-10-26 1983-04-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag